Olefinic polymer, and method for preparing same
AssigneeHanwha Solutions Corporation
InventorsJisong Jo, Jeong Hyun Park, Sung Dong Kim, Munhee Lee, Ui Gap Joung
Life of this patent
Estimating the term…
Loading patent…
AssigneeHanwha Solutions Corporation
InventorsJisong Jo, Jeong Hyun Park, Sung Dong Kim, Munhee Lee, Ui Gap Joung
Estimating the term…
An olefinic polymer and a method for preparing the olefinic polymer are disclosed. The olefinic polymer has excellent melt strength, and thus has excellent bubble stability during blown film molding. The olefinic polymer has (1) a density of 0.9 to 0.95 g/cm3; (2) a melt index (I2.16) of 0.1 to 5.0 g/10 min as measured with a load of 2.16 kg at 190° C.; (3) a ratio between a melt index (I21.6) measured with a load of 21.6 kg and a melt index (I2.16) measured with a load of 2.16 kg at 190° C. (melt flow ratio; MFR) of 20 or more; (4) a melt tension of 55 mN or more at a velocity at break of 350 mm/s; and (5) a maximum velocity at break of 550 mm/s or more.
An olefinic polymer which has (1) a density of 0.9 to 0.95 g/cm3;
A method for preparing an olefinic polymer, the method comprising:
Dependencies are inferred from the claim text.