Methods for making zeolite-Y particles
AssigneeSaudi Arabian Oil Company
InventorsFaisal Alotaibi, Lianhui Ding, Mohammad F. Aljishi
Life of this patent
Estimating the term…
Loading patent…
AssigneeSaudi Arabian Oil Company
InventorsFaisal Alotaibi, Lianhui Ding, Mohammad F. Aljishi
Estimating the term…
A method of making zeolite-Y particles may include dissolving a silica source material into a first solvent to form a first solution and dissolving an alumina source material into a second solvent to form a second solution. The method may also include combining the first solution with the second solution to form a combined mixture. The combined mixture may include a templating agent. The method may include aging the combined mixture for a time period of from 10 hours to 30 hours to form a zeolite precursor solution and heating the zeolite precursor solution at a temperature of from 50° C. to 70° C. to form an intermediate mixture. The method may include heating the intermediate mixture at a temperature of from 80° C. to 120° C. to form the zeolite-Y particles.
A method for making zeolite-Y particles, the method comprising:
Dependencies are inferred from the claim text.