Described is a method for producing a thermoplastic starch, wherein a mixture is extruded comprising starch and a polyol, preferably selected from the group comprising polyethylene glycol, monosaccharides, sugar alcohols and mixtures thereof, in a quantity of 0 to 9.9 wt. % of the mixture, and an epoxide, selected from the group comprising epoxidised vegetable oils, and mixtures thereof, in a quantity of 0.1 to 6 wt. % of the mixture, the mixture further containing an acid, preferably a carboxylic acid selected from the group consisting of citric acid, malic acid or tartaric acid, in a quantity of 0.1 to 1 wt. % of the mixture, and being devoid of polyester urethane. The invention also describes a thermoplastic starch produced in this way, a compound produced with the aid of the thermoplastic starch, and a film produced from such a compound or an injection-moulded item produced from such a compound.
A method for producing thermoplastic starch, comprising extruding a mixture comprising starch and a polyol in a quantity of from 0 to 9.9 wt. % of the mixture, and an epoxidised plant oil in a quantity of from 0.1 to 6 wt. % of the mixture, wherein the mixture also contains an acid in a quantity of from 0.1 to 1 wt. % of the mixture, and is free from polyester urethane, wherein the thermoplastic starch has a bulk density of 70 to 90 g/100 ml.
A compound containing a thermoplastic starch obtainable by a method for producing thermoplastic starch, comprising extruding a mixture comprising starch and a polyol in a quantity of from 0 to 9.9 wt. % of the mixture and an epoxidised plant oil in a quantity of from 0.1 to 6 wt. % of the mixture, wherein the mixture also contains an acid in a quantity of from 0.1 to 1 wt. % of the mixture and is free from polyester urethane, wherein the thermoplastic starch has a bulk density of 70 to 90 g/100 ml.