Abstract
The present application discloses an anti-blue light OCA optical composition for screen and a preparation method thereof, comprising an OCA adhesive body. The OCA adhesive body comprises a first release film, an OCA hybrid blue light barrier film, an optical PET substrate, a silicone film, and a second release film. The first release film comprises the following components by weight: 25-35 parts of nano cobalt oxide.
Claims12
An anti-blue light OCA optical composition for screen comprises an OCA adhesive body, wherein the OCA adhesive body comprises a first release film, an OCA hybrid blue light barrier film, an optical PET substrate, a silicone film, and a second release film;
- wherein the first release film comprises the following components by weight:
- 25-35 parts of nano cobalt oxide, 25-35 parts of o-phenyldimethylamine, 25-35 parts of benzoyl peroxide, and 10-40 parts of hexamethylphosphoramide;
- the OCA hybrid blue light barrier film comprises the following components by weight:
- 20-40 parts of lauryl methacrylate, 20-40 parts of iso-octyl acrylate, and 20-40 parts of blue light barrier agent;
- the optical PET substrate comprises the following components by weight:
- 10-30 parts of benzyl ester material, 10-30 parts of anthocyanin materials, 10-30 parts of silicon nitride, and 10-30 parts of benzophenone;
- the silicone film comprises the following components by weight:
- 40-60 parts of silica gel, and 40-60 parts of hydrophilic polyurethane resin;
- the second release film comprises the following components by weight:
- 25-35 parts of nano cobalt oxide, 25-35 parts by weight of o-phenyldimethylamine, 25-35 parts of benzoyl peroxide, and 10-40 parts of hexamethylphosphoramide.