Back to results
US 12,679,769 B2Granted
Rejuvenating compounds in high performance asphalt compositions with high recycled content
AssigneeCargill, Incorporated
InventorsTodd Kurth, Scott Nivens, Christopher Stevermer, Anthony Joseph Sylvester, Hassan Tabatabaee
Life of this patent
Estimating the term…
Abstract
Described herein is a rejuvenated asphalt and a method of rejuvenating asphalt comprising mixing a rejuvenator, bitumen, and aggregate to obtain an asphalt mixture, wherein the rejuvenator is present in an amount ranging from about 0.1-40 wt % by weight of the bitumen, and wherein at least 35 wt % of the bitumen is derived from recycled asphalt content. The rejuvenated asphalt provides desirable performance.
Claims20
A method, comprising:
- mixing a rejuvenator, bitumen, and aggregate to obtain an asphalt mixture;
- wherein the rejuvenator is a polymerized oil that is polymerized via sulfurization, the rejuvenator is 0.1 wt % to 40 wt % of the bitumen, and the rejuvenator is 0.1 wt % to 30 wt % of the asphalt mixture,
- wherein at least 35 wt % of the bitumen is derived from recycled asphalt content, and
- wherein the asphalt mixture achieves less than 12.5 mm of rutting as determined by Hamburg Wheeltracker test standard in accordance with AASTHO T 324.
1 more element
A rejuvenated asphalt, comprising:
- a rejuvenator, bitumen, and aggregate;
- wherein the rejuvenator is a polymerized oil that is polymerized via sulfurization, the rejuvenator is 0.1 wt % to 40 wt % by weight of the bitumen, and the rejuvenator is 0.1 wt % to 30 wt % of the asphalt mixture,
- wherein at least 35 wt % of the bitumen is derived from recycled asphalt content, and
- wherein the rejuvenated asphalt achieves less than 12.5 mm of rutting as determined by Hamburg Wheeltracker test standard in accordance with AASTHO T 324.