Elastomeric cushioning materials with strain recovery and anti-tack properties
AssigneePurple Innovation, LLC
InventorsDevin Williamson, Michael Wells, Caleb Lundhal, Jose Jacob Chavez
Life of this patent
Estimating the term…
Abstract
The present disclosure is directed to an elastomeric cushioning element. The elastomeric cushioning element may include about 5 wt. % to about 50 wt. % elastomeric polymer network comprising a triblock copolymer having an average molecular weight of about 100,000 Da to about 500,000 Da; and about 50 wt. % to about 95 wt. % plasticizer disposed in the elastomeric polymer network. The plasticizer may include a first plasticizer having an average molecular weight of about 300 Da to about 800 Da and a viscosity at 40° C. of about 20 cSt to about 10,000 cSt.
Claims19
An elastomeric cushioning element comprising:
- about 5 wt. % to about 50 wt. % elastomeric polymer network comprising a triblock copolymer having an average molecular weight of about 100,000 Da to about 500,000 Da;
- and
- about 50 wt. % to about 95 wt. % plasticizer disposed in the elastomeric polymer network;
- wherein the plasticizer comprises a first plasticizer having an average molecular weight of about 300 Da to about 800 Da and a viscosity at 40° C. of about 20 cSt to about 10,000 cSt;
- wherein the plasticizer further comprises a second plasticizer having a molecular weight of about 200 Da to about 500 Da and a viscosity at 40° C. of about 2 cSt to about 20 cSt.
A method of forming an elastomeric material comprising:
- dissolving an elastomeric polymer network comprising a triblock copolymer having a molecular weight of about 100,000 Da to about 500,000 Da in a solvent to form a mixture;
- adding a plasticizer to the mixture, the plasticizer having a molecular weight of about 300 Da to about 800 Da and a viscosity at 40° C. of about 100 cSt to about 10,000 cSt;
- and
- removing the solvent from the mixture to form the elastomeric material.