# US 12,649,657 B2 · Production of boron nitride nanosheets

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 12,649,657 B2
- Document ID: US12649657B2
- Status: Granted
- Kind: B2
- Application number: 18/245,830
- Filed: 2021-09-02
- Published: 2024-01-25
- Granted: 2026-06-09
- Earliest claimed: 2020-09-21
- Assignees: Deakin University
- Applicants: Deakin University
- Inventors: Luhua Li
- Web page: https://patentgrep.com/patent/US12649657B2

## CPC

- C01B 21/0648: {After-treatment, e.g. grinding, purification (transformation of hexagonal into cubic or wurtzitic boron nitride C04B35/5831)}
- B02C 17/06: with several compartments
- B02C 17/10: with one or a few disintegrating members arranged in the container
- B02C 17/20: Disintegrating members
- C01B 21/064: with boron
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B82Y 40/00: Manufacture or treatment of nanostructures
- C01P 2004/24: Nanoplates, i.e. plate-like particles with a thickness from 1-100 nanometer
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- B02C: CRUSHING, PULVERISING, OR DISINTEGRATING IN GENERAL; MILLING GRAIN ({household tools and machines for pulverising foodstuffs, e.g. coffee and spice mills A47J42/00; pharmaceutical mortars A61J3/02; mechanical processing of refuse and garbage B03B9/06; dressing mould materials by grinding B22C5/04}; obtaining metallic powder by crushing, grinding or milling B22F9/04; {recovery of plastics by disintegrating B29B17/00; crushing raw materials in starch making C08B30/02; beaters for papermaking D21D1/02; crushing devices specially for transport in mines E21F13/002; slag crushing devices F23J1/00; fuel milling devices in combustion apparatus F23K1/00; household devices for crushing coal F24B15/02; ice disintegrating devices F25C5/02})
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

A method of producing boron nitride nanosheets comprising: milling a hexagonal boron nitride crystal material in a ball mill to exfoliate substantially two-dimensional nanosheets from the boron nitride crystal material, wherein ball milling is undertaken within a viscous liquid ball milling medium having a viscosity of 100 to 100,000 mPa·s.

## Claims

### Claim 1

A method of producing boron nitride nanosheets, comprising:
milling a hexagonal boron nitride crystal material in a ball mill to exfoliate substantially two-dimensional nanosheets from the boron nitride crystal material,
wherein ball milling is undertaken within a viscous liquid ball milling medium having a viscosity of 100 to 100,000 mPa·s.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the viscous liquid ball milling medium has a viscosity selected from the group consisting of: 200 to 50000 mPa·s, 500 to 20000 mPa·s, 1000 to 20000 mPa·s, and 1000 to 10000 mPa· s.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the viscous liquid ball milling medium is selected from the group consisting of:
(i) a high viscosity liquid;
(ii) a high viscosity solution using a high molecular weight organic solute dissolved in a solvent; and
(iii) a material melted to form a molten milling medium.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the high viscosity liquid comprises a syrup or polyethylene glycol.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the high viscosity liquid comprises a sugar syrup.

### Claim 6 (depends on 3)

The method according to claim 3, wherein the high viscosity solution comprises polyvinyl alcohol or polyacrylamide dissolved in water, ethanol or another suitable solvent.

### Claim 7 (depends on 3)

The method according to claim 3, wherein the molten milling medium comprises a molten polymer.

### Claim 8 (depends on 1)

The method according to claim 1, further comprising controlling the temperature of the milling medium during ball milling to provide a desired viscosity during ball milling.

### Claim 9 (depends on 1)

The method according to claim 1, wherein ball milling is undertaken using ball milling balls and/or ball milling vessel comprising a polymer material.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the polymeric material of the ball milling balls and/or ball milling vessel is selected from the group consisting of: plastic, rubber, nylon, polyethylene, acetal, and polystyrene.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the ball mill is selected from the group consisting of: a traditional ball mill; a planetary ball mill; and an agitated ball mill.

### Claim 12 (depends on 1)

The method according to claim 1, further comprising the step of:
applying an ultrasonic vibration to the viscous ball milling medium during milling;
wherein the ultrasonic vibration has a frequency selected from a group consisting of: 18 to 200 kHz, 18 to 180 kHz, and 18 to 150 kHz.

### Claim 13 (depends on 1)

The method according to claim 1, wherein ball milling is conducted under an air atmosphere or inert atmosphere mixture.