# US 12,637,393 B2 · Advanced coating chemistries for CMCS

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 12,637,393 B2
- Document ID: US12637393B2
- Status: Granted
- Kind: B2
- Application number: 17/929,255
- Filed: 2022-09-01
- Published: 2024-03-07
- Granted: 2026-05-26
- Earliest claimed: 2022-09-01
- Assignees: ROLLS-ROYCE plc
- Applicants: Rolls-Royce Corporation
- Inventors: Gregory John Kenneth Harrington; Li Li; Robert Alexander Sean Golden
- Web page: https://patentgrep.com/patent/US12637393B2

## CPC

- C04B 41/009: {characterised by the material treated}
- C04B 41/85: with inorganic materials
- C04B 41/4582: {Porous coatings, e.g. coating containing porous fillers}
- C04B 41/5024: {Silicates (C04B41/5022 takes precedence; silico-fluorides C04B41/5018)}
- C04B 41/52: Multiple coating or impregnating {multiple coating or impregnating with the same composition or with compositions only differing in the concentration of the constituents, is classified as single coating or impregnation}
- C04B 41/89: for obtaining at least two superposed coatings having different compositions
- F01D 5/282: {Selecting composite materials, e.g. blades with reinforcing filaments}
- F01D 5/284: {Selection of ceramic materials}
- F01D 5/288: {Protective coatings for blades}
- F01D 11/08: for sealing space between rotor blade tips and stator (specially-shaped blade tips therefor F01D5/20)
- F01D 25/007: {Preventing corrosion}
- F23R 3/007: {constructed mainly of ceramic components}
- C04B 2111/00982: {as construction elements for space vehicles or aeroplanes}
- C04B 2235/402: Aluminium
- C04B 2235/96: Properties of ceramic products, e.g. mechanical properties such as strength, toughness, wear resistance
- F05D 2240/11: Shroud seal segments
- F05D 2300/15: Rare earth metals, i.e. Sc, Y, lanthanides
- F05D 2300/2102: Glass
- F05D 2300/211: Silica
- F05D 2300/2112: Aluminium oxides
- F05D 2300/222: Silicon
- F05D 2300/6033: Ceramic matrix composites [CMC]
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- F01D: NON-POSITIVE DISPLACEMENT MACHINES OR ENGINES, e.g. STEAM TURBINES (machines or engines for liquids F03; non-positive displacement pumps F04D)
- F23R: GENERATING COMBUSTION PRODUCTS OF HIGH PRESSURE OR HIGH VELOCITY, e.g. GAS-TURBINE COMBUSTION CHAMBERS (fluidised bed combustion apparatus specially adapted for operation at superatmospheric pressures F23C10/16)
- F05D: INDEXING SCHEME FOR ASPECTS RELATING TO NON-POSITIVE-DISPLACEMENT MACHINES OR ENGINES, GAS-TURBINES OR JET-PROPULSION PLANTS

## Abstract

An article having a coating system configured to inhibit or prevent crystallization of TGO at the operating temperature of the article. An article includes a substrate defining a surface and a coating layer that includes a dopant configured to inhibit crystallization of amorphous silicon dioxide thermally grown oxide on the bond coat at an operating temperature of the article. The dopant includes a glass modifier. By inhibiting or preventing TGO crystallization, the described coating systems may increase a useable life of the component.

## Claims

### Claim 1

An article comprising:
a substrate defining a surface; and
a coating layer overlying the substrate, wherein the coating layer comprises a dopant configured to inhibit crystallization of amorphous silicon dioxide thermally grown oxide (TGO) between the coating layer and the substrate at an operating temperature of the article,
wherein:
the dopant comprises a glass modifier,
the dopant is configured to migrate into the TGO to form a bilayer TGO comprising an amorphous first region on a crystalline second region, and
the dopant is present in a concentration sufficient to stabilize the amorphous first region as a hermetic barrier during thermal cycling of the article through a temperature of 180° C. to 300° C., thereby inhibiting spallation of the coating layer caused by volume contraction of the crystalline second region during a B-cristobalite to a-cristobalite phase transformation.

### Claim 2 (depends on 1)

The article of claim 1, wherein the glass modifier comprises one or more of aluminum, sodium, potassium, calcium, iron, or one or more rare-earth elements.

### Claim 3 (depends on 1)

The article of claim 1, wherein the coating layer is a bond coat layer.

### Claim 4 (depends on 1)

The article of claim 1, wherein the coating layer comprises an environmental barrier coating (EBC) further comprising at least one rare-earth monosilicate or rare-earth disilicate.

### Claim 5 (depends on 1)

The article of claim 1, further comprising a bond coat on a surface of the substrate and between the coating layer and the surface of the substrate.

### Claim 6 (depends on 1)

The article of claim 1, wherein the coating layer comprises an environmental barrier coating (EBC) further comprising at least one rare-earth monosilicate or rare-earth disilicate.

### Claim 7 (depends on 1)

The article of claim 1, wherein the dopant comprises one or more compounds, and the one or more compounds comprise at least one of Al2O3, Na2O, K2O, Na2Al2O4, AlSi, CaO, Fe2O3, Y2O3, Yb2O3, or mixtures or combinations thereof.

### Claim 8 (depends on 5)

The article of claim 5, wherein the coating layer on the bond coat is part of the bond coat and forms a first region of the bond coat on a second region of the bond coat, and wherein the first region of the bond coat includes a greater amount of the dopant than the second region.

### Claim 9 (depends on 1)

The article of claim 1, wherein the dopant comprises aluminum, sodium, and potassium.

### Claim 10 (depends on 9)

The article of claim 9, wherein the dopant comprises more aluminum than potassium or sodium.

### Claim 11 (depends on 2)

The article of claim 2, wherein the dopant comprises at least two of aluminum, sodium, potassium, ytterbium, calcium, or iron.

### Claim 12 (depends on 1)

The article of claim 1, wherein coating layer comprises between about 0.1 mole percent (mol %) and about 15 mol % of the dopant.

### Claim 13 (depends on 1)

The article of claim 1, wherein the coating layer comprises at least 2 mol % percent aluminum.

### Claim 14 (depends on 1)

The article of claim 1, further comprising an abradable coating on the coating layer, wherein the abradable coating comprises at least one rare-earth monosilicate or rare-earth disilicate.

### Claim 15 (depends on 1)

The article of claim 1, wherein the coating layer comprises graded chemistry, a graded porosity, or a graded chemistry and a graded porosity.

### Claim 16 (depends on 1)

The article of claim 1, wherein the article is a high temperature component of a gas turbine engine.

### Claim 17

A gas turbine engine component comprising:
a ceramic matrix composite (CMC) substrate defining at least a portion of the gas turbine engine component, wherein the CMC substrate comprises a silicon-containing material; and
a coating layer overlying the CMC substrate, wherein the coating layer comprises a dopant configured to inhibit crystallization of amorphous silicon dioxide thermally grown oxide (TGO) between the coating layer and the CMC substrate at an operating temperature of the gas turbine engine component,
wherein:
the dopant comprises a glass modifier, and
the dopant is configured to migrate into the TGO to maintain at least a portion of the TGO in an amorphous phase that is substantially continuous and forms a hermetic barrier configured to reduce migration of oxidizing species into the CMC substrate while the component is thermally cycled through a temperature of 270° C.

### Claim 18 (depends on 17)

The gas turbine engine component of claim 17, wherein the glass modifier comprises one or more of aluminum, sodium, potassium, calcium, iron, or one or more rare-earth elements.

### Claim 19

A method comprising:
depositing a coating layer formulation on a substrate defining a surface to form a coating layer,
wherein the coating layer comprises a dopant configured to inhibit crystallization of an amorphous silicon dioxide thermally grown oxide (TGO) between the coating layer and the substrate at an operating temperature of an article;
wherein:
the dopant comprises a glass modifier the dopant comprises a glass modifier,
the dopant is configured to migrate into the TGO to form a bilayer TGO comprising an amorphous first region on a crystalline second region, and
the dopant is present in a concentration sufficient to stabilize the amorphous first region as a hermetic barrier during thermal cycling of the article through a temperature of 180° C. to 300° C., thereby inhibiting spallation of the coating layer caused by volume contraction of the crystalline second region during a β-cristobalite to α-cristobalite phase transformation.

### Claim 20 (depends on 19)

The method of claim 19, wherein the glass modifier comprises one or more of aluminum, sodium, potassium, calcium, iron, or one or more rare-earth elements.