Soft magnetic alloy powder, magnetic core, magnetic component and electronic device
AssigneeTDK Corporation
InventorsYoshiki Kajiura, Akito Hasegawa, Kazuhiro Yoshidome, Hiroyuki Matsumoto, Hironobu Kumaoka
Life of this patent
Estimating the term…
Abstract
A soft magnetic alloy powder has a specific composition in which a Co content is large. A soft magnetic alloy powder has a glass transition point Tg and a melting point Tm, 900° C.≤Tm≤1200° C. is satisfied, or when coercivity when applying a pressure XP to a soft magnetic alloy powder is set as YH, and a straight line obtained by linearly approximating a relationship between XP and YH by a method of least squares is set as YH=kXP+1, k (unit: Oe/MPa) satisfies 0≤k≤0.00100.
Claims9
A soft magnetic alloy powder comprising:
- a main component having a composition formula of
- (Co(1−(α+β))X1αX2β)(1−(a+b+c+d+e+f))MaBbPcSidCreSf(atom number ratio),
- wherein X1 represents one or more selected from the group consisting of Fe and Ni,
- X2 represents one or more selected from the group consisting of Al, Mn, Ag, Zn, Sn, As, Sb, Cu, Bi, N, O, C, and rare-earth elements,
- M represents one or more selected from the group consisting of Nb, Hf, Zr, Ta, Mo, W, Ti, and V,
- 0.001≤a≤0.140,
- 0.180≤b≤0.220,
- 0.010≤c≤0.050,
- 0≤d≤0.250,
- 0≤e≤0.030,
- 0≤f≤0.010,
- 0.160≤b+c+d+e+f≤0.430,
- 0.500<1−(a+b+c+d+e+f)<0.840,
- α≥0,
- β≥0, and
- 0≤α+β<0.50 are satisfied,
- the soft magnetic alloy powder has a glass transition point Tg and a melting point Tm,
- 900° C.≤Tm≤1200° C. is satisfied, and
- a coercivity He of the soft magnetic alloy powder is 0.04 Oe or less.