A method for producing agent an embossing die for texturing an embossable material surface of a decorative laminate:
- providing a carrier material made of paper and/or plastic, said carrier having a thickness of from 50 to 200 μm;
- applying a UV-curable lacquer layer of acrylated oligomer onto the carrier material,
- forming a three-dimensional embossed structure into the lacquer layer applied to the carrier material, and
- curing the lacquer layer by irradiation with UV light during the forming of the embossed structure,
- wherein before the UV-curable lacquer layer is applied, at least one adhesion promoter layer comprising acrylated oligomer, a reactive diluent and a photo initiator which reacts to UV radiation, is applied onto the carrier material, and the lacquer layer having the embossed structure is cured by irradiation with UV light, to such an extent that,
- when finished curing, the surface of the lacquer layer of the embossing die having the embossed structure has an average Martens hardness according to DIN EN ISO 14577 in the range from 10 to 80 N/mm2,
- and, after curing, the lacquer layer having the embossed structure has an average roughness depth (Rz) according to DIN EN ISO 4287 of from 10 to 200 μm.