Back to results
US 12,605,769 B2Granted
Insert and cutting tool
AssigneeKYOCERA Corporation
InventorsHiroyuki Nanahara, Futoshi Isobe, Yusuke Nagaoka
Life of this patent
Estimating the term…
Abstract
An insert of the present disclosure includes a cBN sintered compact containing cBN and TiN. The cBN occupies 60% or more of the cross-sectional area of the cBN sintered compact observed. TiN (200) is higher than cBN (111), where the TiN (200) is an X-ray intensity on a (200) plane of the TiN and the cBN (111) is an X-ray intensity on a (111) plane of the cBN, obtained by X-ray diffraction on the cBN sintered compact.
Claims8
An insert, comprising a cBN sintered compact containing cBN and TiN, wherein
- the cBN occupies 60% or more of a cross-sectional area of the cBN sintered compact observed, and
- TiN (200) is higher than cBN (111), where the TIN (200) is an X-ray intensity on a (200) plane of the TiN and the cBN (111) is an X-ray intensity on a (111) plane of the cBN, obtained by X-ray diffraction on the cBN sintered compact, wherein
- the cBN sintered compact comprises a binder phase, and
- the binder phase contains 0.5-3.0 atomic % of Al.
1 more element
A cutting tool, comprising:
- a holder having a rod-shape and comprising a pocket at an end portion of the rod-shaped holder;
- and
- an insert located in the pocket, the insert comprising a cBN sintered compact containing cBN and TiN, wherein
- the cBN occupies 60% or more of a cross-sectional area of the cBN sintered compact observed, and
- TiN (200) is higher than cBN (111), where the TiN (200) is an X-ray intensity on a (200) plane of the TiN and the cBN (111) is an X-ray intensity on a (111) plane of the cBN, obtained by X-ray diffraction on the cBN sintered compact,
- the cBN sintered compact comprises a binder phase, and
- the binder phase contains 0.5-3.0 atomic % of Al.