Disclosed herein are compositions and methods relating to fine aggregate for a Controlled Low-Strength Material (CLSM) recycled from a consumer waste stream of bottle glass. Such disclosed compositions may be advantageous, for example, for backfilling trenches in street cuts for utility repairs or new utility installations, such as digital cables. The disclosed compositions that incorporate the recycled glass aggregate into a CLSM that achieves satisfactory compressive strengths. The disclosed compositions are not negatively impacted by Alkali-Silica Reactivity causing expansion.
Claims26
A composition for a controlled low-strength materials concrete comprising:
- between 60% and 95% aggregate by weight of the composition, wherein the aggregate comprises glass;
- between 3% and 25% Portland cement by weight of the composition;
- and
- between 5% and 40% water by weight of the composition;
- the composition having a compressive strength of between 20 psi and 2000 psi after 7 days, and the composition having a compressive strength between 15 psi and 2000 psi after 28 days.