Method for detecting corrosion severity of a metallic surface on a pipeline
OwnerHomero Castaneda-Lopez, Lin Cheninventors
Life of this patent
Estimating the term…
Abstract
Provided herein are non-invasive and non-destructive methods for classifying the type of external corrosion defect and the severity thereof in the cathodic protection system on a buried pipeline. Mathematical tools and algorithms are utilized to classify the type and the severity of the corrosion defect.
Claims11
A non-invasive and non-destructive inspection method for detecting and classifying coating failures on a buried metallic pipeline, consisting of:
- a) selecting an inspection area on the coating on the buried metallic pipeline;
- said coating comprising part of a cathodic protection system for the buried metallic pipeline;
- b) disconnecting a continuous cathodic protection of the buried metallic pipeline;
- c) producing a profile of a change in the cathodic protection based on a polarization decay thereof at the inspection area over a period of time;
- d) correlating the profile with a coating failure or lack thereof at the inspection area via a comparison to a corrosion severity database;
- e) classifying a severity of the coating failure as an active surface failure, an active surface with pitting failure, a bare metallic surface failure, or a passive surface failure;
- and
- f) selecting at least one additional inspection area on the buried metallic pipeline and repeating the method steps b) to e) to produce at least one additional profile.
A method for classifying a severity of a corrosion defect on an external coating on a buried metallic pipeline, consisting of:
- in a non-invasive and non-destructive process:
- a) selecting a test point on the external coating disposed on the buried metallic pipeline, said external coating comprising part of a cathodic protection system;
- b) switching off voltage to the cathodic protection system on the buried metallic pipeline;
- c) acquiring an instantaneous potential relaxation at a plurality of acquisition times at the test point;
- d) producing a potential relaxation curve from the acquired instantaneous potential relaxation at the plurality of acquisition times;
- e) comparing the potential relaxation curve to a database of potential relaxation curves of a severity level of the corrosion defect;
- f) classifying the severity level of the corrosion defect as active dissolution, pitting, passive, or no corrosion;
- and
- g) selecting at least one additional test point on the buried metallic pipeline and repeating the method steps b) to f).
A non-invasive and non-destructive inspection method for a buried metallic pipeline with a cathodic protection system, consisting of:
- selecting a plurality of inspection places along an external coating disposed on the buried metallic pipeline;
- wherein the external coating is part of the cathodic protection system;
- turning off the cathodic protection system to the metallic pipeline;
- recording a potential relaxation curve from a plurality of instantaneous relaxation voltages each acquired at a predetermined time point for each of the plurality of inspection places;
- comparing each of the potential relaxation curves to a database of potential relaxation curves that are correlated with a severity level of corrosion;
- and
- identifying each of the plurality of inspection places on the external coating on the buried pipeline as comprising the severity level of corrosion that is active dissolution, pitting or passive or without corrosion.
Dependencies are inferred from the claim text.