Method of treating a cemented carbide mining insert
AssigneeSandvik Mining and Construction Tools AB
InventorsMirjam Lilja, Jose Luis Garcia, Andreas Blomqvist, Ioannis Arvanitidis, Erik Holmstrom
Life of this patent
Estimating the term…
Loading patent…
AssigneeSandvik Mining and Construction Tools AB
InventorsMirjam Lilja, Jose Luis Garcia, Andreas Blomqvist, Ioannis Arvanitidis, Erik Holmstrom
Estimating the term…
A method of redistributing the binder phase of a cemented carbide mining insert having a WC hard-phase component, optionally one or more further hard-phase components and a binder includes the steps of providing a green cemented carbide mining insert; applying at least one binder puller selected from a metal oxide or a metal carbonate to only at least one local area of the surface of the green cemented carbide insert; sintering the green carbide mining insert to form a sintered cemented carbide insert; and subjecting the sintered cemented carbide insert to dry tumbling process executed at an elevated temperature of or above 100° C., preferably at a temperature of or above 200° C., more preferably at a temperature of between 200° C. and 450° C.
A method of redistributing a binder phase of a cemented carbide mining insert having a WC hard-phase component, optionally one or more further hard-phase components and a binder, the method comprising the steps of:
Dependencies are inferred from the claim text.