Nickel-based alloy having superior surface properties and production method for the same
AssigneeNippon Yakin Kogyo Co., Ltd.
InventorsDaiki Ogasawara, Fumiaki Kirihara
Life of this patent
Estimating the term…
Loading patent…
AssigneeNippon Yakin Kogyo Co., Ltd.
InventorsDaiki Ogasawara, Fumiaki Kirihara
Estimating the term…
A composition of non-metallic inclusions that affect surface properties and provides Ni-based alloys with superior surface properties. A Ni-based alloy consisting of: all by mass %, Ni: 52.0% or more, C: 0.001% to 0.030%, Si: 0.01 to 0.10%, Mn: 0.10 to 1.50%, P: 0.030% or less, S: 0.0050% or less, Cr: 13.0 to 25.0%, Mo: 10.0 to 18.0%, W: 1.00 to 5.00%, Cu: 1.00% or less, Co: 3.00% or less, Al: 0.001 to 0.170%, Fe: 2.00 to 8.00%, Mg: 0.0010 to 0.0200%, Ca: 0.0001 to 0.0040%, V: 0.500% or less, Nb: 0.001 to 0.100%, O: 0.0001 to 0.0050%, wherein the non-metallic inclusions includes one or more of MgO, CaO, CaO—MgO-based oxides, CaO—Al2O3—MgO-based oxides, and MgO.Al2O3, the MgO.Al2O3 has number ratio of 50% or less with all oxide-based non-metallic inclusions.
A Ni-based alloy consisting of, all by mass %:
A Ni-based alloy comprising, all by mass %:
Dependencies are inferred from the claim text.