Honeycomb structure and exhaust gas purifying device
AssigneeNGK Insulators, Ltd.
InventorsKazuya Hosoda, Takafumi Kimata, Yunie Izumi, Takuya Nakashima
Life of this patent
Estimating the term…
Abstract
A pillar shaped honeycomb structure includes: an outer peripheral wall; and porous partition walls disposed on an inner side of the outer peripheral wall, the partition walls defining a plurality of cells, each of the cells penetrating from one end face to other end face to form a flow path, wherein at least one cell of the cells has a magnetic substance coated with glass.
Claims15
A pillar shaped honeycomb structure, comprising:
- an outer peripheral wall;
- and
- porous partition walls disposed on an inner side of the outer peripheral wall, the partition walls defining a plurality of cells, each of the cells penetrating from one end face to other end face to form a flow path,
- wherein at least one cell of the cells has a magnetic substance coated with glass,
- the magnetic substance coated with the glass is provided in a form of a layer on surfaces of the partition walls in the cell to form a coating layer,
- the coating layer has an open porosity of 40 to 90%,
- the glass coating the magnetic substance has a thickness of 1 to 10 μm, and
- a ratio of a thermal expansion coefficient α1 of the magnetic substance to a thermal expansion coefficient α2 of the glass:
- α1/α2 is 0.8 to 1.2.
6 more elements
A pillar shaped honeycomb structure, comprising:
- an outer peripheral wall;
- and
- porous partition walls disposed on an inner side of the outer peripheral wall, the partition walls defining a plurality of cells, each of the cells penetrating from one end face to other end face to form a flow path,
- wherein at least one cell of the cells has a magnetic substance coated with glass,
- the magnetic substance coated with the glass is filled in the cell,
- the glass coating the magnetic substance has a thickness of 1 to 10 μm, and
- a ratio of a thermal expansion coefficient α1 of the magnetic substance to a thermal expansion coefficient α2 of the glass:
- α1/α2 is 0.8 to 1.2.
5 more elements
Dependencies are inferred from the claim text.