# US 12,503,549 B2 · Biaxially-stretched polyester resin film and manufacturing method for same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 12,503,549 B2
- Document ID: US12503549B2
- Status: Granted
- Kind: B2
- Application number: 17/915,219
- Filed: 2021-03-26
- Published: 2023-04-13
- Granted: 2025-12-23
- Earliest claimed: 2020-03-31
- Assignees: Unitika Ltd.
- Applicants: Unitika Ltd.; Nippon Ester Co., Ltd.; Unitika Trading Co., Ltd.
- Inventors: Goro Araki; Hiroshi Ashihara; Hazumu Nagano
- Web page: https://patentgrep.com/patent/US12503549B2

## CPC

- C08G 63/183: Terephthalic acids
- C08L 67/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds (C08L67/06 takes precedence)
- B29C 55/12: biaxial
- C08G 63/78: Preparation processes
- C08J 5/18: Manufacture of films or sheets
- C08J 2300/30: Polymeric waste or recycled polymer
- C08J 2467/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds (C08J2467/06 takes precedence)
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2205/03: containing three or more polymers in a blend
- Y02W 30/62: Plastics recycling; Rubber recycling
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

To provide a biaxially stretched polyester resin film that has excellent properties equal to or better than those of biaxially stretched polyester film that does not use recycled raw material, and in particular that has an excellent flexural resistance in low-temperature environments. A biaxially stretched polyester resin film that characteristically satisfies both of the following properties (1) and (2): (1) in differential scanning calorimetry (DSC), after heating from 25° C. to 300° C. at a heating rate of 20° C./minute and holding for 10 minutes at 300° C., the temperature of crystallization during cooling at a cooling rate of 40° C./minute is 160° C. to 180° C.; and (2) the number of pinholes after the execution of 200 repetitive cycles of a flexural fatigue test in a −10° C. atmosphere using a Gelbo Flex Tester is not more than 10/500 cm2.

## Claims

### Claim 1

A biaxially stretched polyester resin film characterized in that the film satisfies the following properties (1), (2), and (3):
(1) in differential scanning calorimetry (DSC), after heating the film from 25° C. to 300° C. at a heating rate of 20° C./minute and holding for 10 minutes at 300° C., the temperature of crystallization during cooling at a cooling rate of 40° C./minute is 160° C. to 180° C.;
(2) a number of pinholes after the execution of 200 repeating cycles of a flexural fatigue test in a −10° C. atmosphere using a Gelbo Flex Tester is not more than 10/500 cm2; and
(3) a concentration of carboxyl end groups is 20 to 60 eq/t.

### Claim 2 (depends on 1)

The biaxially stretched polyester resin film according to claim 1, wherein a haze of the film is not more than 10.0%.

### Claim 3 (depends on 1)

The biaxially stretched polyester resin film according to claim 1, wherein a surface crystallinity as determined by infrared spectroscopic analysis (ATR-IR) using a total reflection measurement method is 1.1 to 1.4.

### Claim 4 (depends on 1)

The biaxially stretched polyester resin film according to claim 1, having a thickness of not more than 50 μm and having a tensile elongation in both the MD direction and TD direction of at least 100%.

### Claim 5 (depends on 1)

The biaxially stretched polyester resin film according to claim 1, having a b* value of 0 or less.