Back to results
US 12,489,106 B2Granted
Method for the manufacture of electrodes
AssigneesSyensqo SA, Politecnico Di Torino
InventorsJulio A. Abusleme, Maurizio Biso, Alberto Frache, Daniele Battegazzore, Francesco Liberale
Life of this patent
Estimating the term…
Abstract
The present invention pertains to an electrode-forming composition, to use of said electrode-forming composition in a process for the manufacture of an electrode, to said electrode and to an electrochemical device comprising said electrode.
Claims15
A composition [composition (C)] comprising:
- from 0.5 wt. % to less than 20 wt. % of at least one semi-crystalline partially fluorinated polymer [polymer (F)] comprising recurring units derived from 1,1-difluoroethylene (VDF) and recurring units derived from at least one hydrogenated monomer comprising at least one carboxylic acid end group [monomer (MA)];
- from 10 wt. % to less than 60 wt. % of at least one liquid medium [medium (L)] characterized by a boiling point equal to or higher than 150°° C., wherein said medium (L) is selected from the group consisting of organic carbonates, ionic liquids (IL), or combinations thereof;
- and
- at least 50 wt. % of at least one electro-active compound [compound (EA)];
- wherein the above amounts are based on the total weight of said composition (C), and wherein said polymer (F) is characterized by an intrinsic viscosity higher than 0.05 L/g, the intrinsic viscosity being measured from the dropping time of a solution of said polymer (F) at 25° C. at a concentration of 0.2 g/dl in N.N-dimethylformamide using a Ubbelhode viscosimeter, and
- wherein the composition (C) is free from any polar solvent [solvent(S)].
3 more elements
A process for the manufacture of an assembly, said process comprising:
- (i) providing a substrate;
- (ii) providing composition (C) comprising:
- from 0.5 wt. % to less than 20 wt. % of at least one semi-crystalline partially fluorinated polymer [polymer (F)] comprising recurring units derived from 1,1-difluoroethylene (VDF);
- from 10 wt. % to less than 60 wt. % of at least one liquid medium [medium (L)] characterized by a boiling point equal to or higher than 150° C., wherein said medium (L) is selected from the group consisting of organic carbonates, ionic liquids (IL), or combinations;
- at least 50 wt. % of at least one electro-active compound [compound (EA)];
- wherein the above amounts are based on the total weight of said composition (C), and
- wherein said polymer (F) is characterized by an intrinsic viscosity higher than 0.05 L/g, the intrinsic viscosity being measured from the dropping time of a solution of said polymer (F) at 25° C. at a concentration of 0.2 g/dL in N.N-dimethylformamide using a Ubbelhode viscosimeter;
- and
- wherein the composition (C) is free from any polar solvent [solvent(S)];
- (iii) heating said composition (C) at a temperature higher than 100° C.;
- (iv) extruding the composition (C) provided in step (ii) onto the substrate provided in step (i), thereby providing an assembly comprising a substrate coated with at least one layer consisting of said composition (C).