Removable moisture barrier
AssigneeAmerican Sealants, Inc.
InventorsAndrew Zaremba, Whitney Bolt, Robert K. Ddamulira
Life of this patent
Estimating the term…
Abstract
A moisture barrier composition includes polymer resin 10 weight percent (wt. %) to 50 wt. %, plasticizer 10 wt. % to 50 wt. %, pigment 0.01 wt. % to 2 wt. %, liquid heat and UV stabilizer 0.01 wt. % to 2 wt. %, anti-settling agent 0.01 wt. % to 2 wt. % or thickening agent 0.5 wt. % to 5 wt. %, a first filler 5 wt. % to 50 wt. %, a second filler 5 wt. % to 50 wt. %, moisture scavenger 0.5 wt. % to 5 wt. %, and catalyst 0.01 wt. % to 2 wt.
Claims20
A moisture barrier composition, comprising:
- polymer resin 10 weight percent (wt. %) to 50 wt. %;
- plasticizer 10 wt. % to 50 wt. %;
- pigment 0.01 wt. % to 2 wt. %;
- liquid heat and UV stabilizer 0.01 wt. % to 2 wt. %;
- anti-settling agent 0.01 wt. % to 2 wt. % or thickening agent 0.5 wt. % to 5 wt. %;
- a first filler 5 wt. % to 50 wt. %;
- a second filler 5 wt. % to 50 wt. %;
- moisture scavenger 0.5 wt. % to 5 wt. %;
- and
- catalyst 0.01 wt. % to 2 wt. %.
A moisture barrier formed by a process, the process comprising:
- applying a moisture barrier composition to a surface, wherein the moisture barrier composition comprises:
- polymer resin 10 weight percent (wt. %) to 50 wt. %;
- plasticizer 10 wt. % to 50 wt. %;
- pigment 0.01 wt. % to 2 wt. %;
- liquid heat and UV stabilizer 0.01 wt. % to 2 wt. %;
- anti-settling agent 0.01 wt. % to 2 wt. % or thickening agent 0.5 wt. % to 5 wt. %;
- a first filler 5 wt. % to 50 wt. %;
- a second filler 5 wt. % to 50 wt. %;
- moisture scavenger 0.5 wt. % to 5 wt. %;
- and
- catalyst 0.01 wt. % to 2 wt. %;
- and
- curing the applied moisture barrier composition by exposing it to moisture.
A method of using a moisture barrier comprising:
- applying a moisture barrier composition to a surface, wherein the moisture barrier composition comprises:
- polymer resin 10 weight percent (wt. %) to 50 wt. %;
- plasticizer 10 wt. % to 50 wt. %;
- pigment 0.01 wt. % to 2 wt. %;
- liquid heat and UV stabilizer 0.01 wt. % to 2 wt. %;
- anti-settling agent 0.01 wt. % to 2 wt. % or thickening agent 0.5 wt. % to 5 wt. %;
- a first filler 5 wt. % to 50 wt. %;
- a second filler 5 wt. % to 50 wt. %;
- moisture scavenger 0.5 wt. % to 5 wt. %;
- and
- catalyst 0.01 wt. % to 2 wt. %;
- and
- curing the applied moisture barrier composition by exposing it to moisture.
Dependencies are inferred from the claim text.