# US 12,460,100 B2 · Polymer latex for the preparation of an elastomeric film having excellent stress retention properties and softness

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 12,460,100 B2
- Document ID: US12460100B2
- Status: Granted
- Kind: B2
- Application number: 17/760,670
- Filed: 2020-09-18
- Published: 2022-10-20
- Granted: 2025-11-04
- Earliest claimed: 2019-09-20
- Assignees: Synthomer Sdn. Bhd.
- Applicants: Synthomer Sdn. Bhd.
- Inventors: Zhenli Wei; Yi-Fan Goh; Zuraida Mohamad
- Web page: https://patentgrep.com/patent/US12460100B2

## CPC

- C09D 109/04: Latex
- C08F 2/22: Emulsion polymerisation
- C08F 212/10: with nitriles
- C08F 220/06: Acrylic acid; Methacrylic acid; Metal salts or ammonium salts thereof
- C08F 220/44: Acrylonitrile
- C08F 220/46: with carboxylic acids, sulfonic acids or salts thereof
- C08F 236/06: Butadiene
- C08F 236/08: Isoprene
- C08F 236/10: with vinyl-aromatic monomers
- C08F 236/12: with nitriles
- C08L 9/04: Latex
- C08L 9/08: Latex
- C08L 13/02: Latex
- C08L 15/00: Compositions of rubber derivatives (C08L11/00, C08L13/00 take precedence)
- C08L 55/02: ABS [Acrylonitrile-Butadiene-Styrene] polymers
- C09D 109/08: Latex
- C09D 113/02: Latex
- C09D 125/10: with conjugated dienes
- C09J 109/04: Latex
- C09J 109/08: Latex
- C09J 113/02: Latex
- C09J 125/10: with conjugated dienes
- A41D 19/0058: {Three-dimensional gloves}
- C08L 9/10: Latex (C08L9/04, C08L9/08 take precedence)
- C08L 25/10: with conjugated dienes
- C08L 53/02: of vinyl-aromatic monomers and conjugated dienes
- C08L 53/025: {modified}
- C09D 109/10: Latex (C09D109/04, C09D109/08 take precedence)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- A41D: OUTERWEAR; PROTECTIVE GARMENTS; ACCESSORIES

## Abstract

A polymer latex is described for the preparation of an elastomeric film obtained by free-radical emulsion polymerization of a mixture of ethylenically unsaturated monomers comprising: a) 15 to 99 wt.-% of conjugated dienes; b) 0 to 80 wt.-% of ethylenically unsaturated nitrile compounds; c) 0 to 70 wt.-% of vinyl aromatic monomers; the sum of ethylenically unsaturated nitrile compounds b) and vinyl aromatic monomers c) being 0.95 to 84.95 wt.-% d) 0.05 to 10 wt.-% of ethylenically unsaturated acids wherein the ethylenically unsaturated acids comprise d1) an ethylenically unsaturated acid comprising an acid functional group; and a spacer group separating the ethylenically unsaturated group and the acid functional group by at least 4 atoms; and e) 0 to 65 wt.-% of co-polymerizable ethylenically unsaturated compounds, wherein monomers a) to e) are as defined.

## Claims

### Claim 1

A polymer latex composition for preparation of an elastomeric film comprising a polymer latex obtained by free-radical emulsion polymerization of a mixture of ethylenically unsaturated monomers comprising:
a) 15 to 99 wt.-% of conjugated dienes;
b) 0 to 80 wt.-% of ethylenically unsaturated nitrile compounds;
c) 0 to 70 wt.-% of vinyl aromatic monomers, the sum of ethylenically unsaturated nitrile compounds b) and vinyl aromatic monomers c) being 0.95 to 84.95 wt.-%;
d) 0.05 to 10 wt.-% of ethylenically unsaturated acids wherein the ethylenically unsaturated acids comprise
d1) an ethylenically unsaturated acid comprising
an acid functional group; and
a spacer group separating the ethylenically unsaturated group and the acid functional group by at least 4 atoms,
wherein the acid functional group is selected from carboxylic acid groups and phosphorous-containing acid groups; and
e) 0 to 65 wt.-% of co-polymerizable ethylenically unsaturated compounds,
wherein monomers a) to e) are different from each other and the weight percentages are based on the total monomers in the mixture,
wherein monomer d) comprises an ethylenically unsaturated carboxylic acid,
wherein the composition further comprises an oxirane functional compound, and
wherein the ethylenically unsaturated acid of d1) is the sole ethylenically unsaturated acid in the mixture of ethylenically unsaturated monomers.

### Claim 2 (depends on 1)

The polymer latex composition according to claim 1, wherein d1) is selected from compounds having the structure:
CHR2═CR1-A-X,
wherein:
R1 is selected from H and C1-C4 alkyl,
R2 is selected from H or -A-X;
A is a divalent spacer group separating the ethylenically unsaturated group and the functional group X by at least 4 atoms independently at each occurrence selected from:
—(C(O)—W)n—Y—(O)m—; —(C(O)—W)n—Y—O—C(O)—Y— and —(CH2)k—O—(C(O))p—Y—(O)m—;
n, m, k and p are integers independently at each occurrence selected from 0 or 1;
W is —O— or —NR3—;
R3 is selected from H and C1-C4 alkyl;
Y is independently at each occurrence selected from optionally substituted linear, branched, cyclic or aromatic C2 to C30 divalent hydrocarbon or hetero hydrocarbon groups;
X is selected from —C(O)OH and —P(O)(OH)2;
with the proviso that if X is —C(O)OH, m is 0;
or -A-X is selected from —C(O)—O—(Y—C(O)—O)l—H, wherein l is an integer from 2 to 10, and
mixtures thereof.

### Claim 3 (depends on 1)

The polymer latex composition according to claim 1, wherein the ethylenically unsaturated acid of d1) is present from 0.1 to 9 wt.-%, based on the total monomers in the mixture.

### Claim 4 (depends on 1)

The polymer latex composition according to claim 1, wherein:
a) the conjugated dienes are selected from butadiene, isoprene, 2,3-dimethyl-1,3-butadiene, 2-ethyl-1,3-butadiene, 1,3-pentadiene, myrcene, ocimene, farnasene and combinations thereof,
b) the ethylenically unsaturated nitrile compounds are selected from (meth)acrylonitrile, alpha-cyanoethyl acrylonitrile, fumaronitrile, alpha-chloronitrile and combinations thereof;
c) the vinyl aromatic monomers are selected from styrene, alpha-methyl styrene, vinyl toluene and combinations thereof; and
e) the co-polymerizable ethylenically unsaturated compounds are selected from
e1) alkyl esters of ethylenically unsaturated acids;
e2) hydroxyalkyl esters of ethylenically unsaturated acids;
e3) amides of ethylenically unsaturated acids;
e4) vinyl carboxylates;
e5) alkoxyalkyl esters of ethylenically unsaturated acids;
e6) monomers having at least two ethylenically unsaturated groups;
e7) ethylenically unsaturated silanes and combinations thereof.

### Claim 5 (depends on 1)

The polymer latex composition according to claim 1, wherein the mixture of ethylenically unsaturated monomers for the polymer latex comprises:
a) 20 to 98 wt.-% of conjugated dienes;
b) 1 to 60 wt.-% of ethylenically unsaturated nitrile compounds;
c) 0 to 40 wt.-% of vinyl aromatic monomers;
d) 1 to 8 wt.-% of ethylenically unsaturated acids;
e1) 0 to 25 wt.-% of C1 to C8 alkyl (meth)acrylates;
e3) 0 to 10 wt.-% of amides of ethylenically unsaturated acids;
e4) 0 to 10 wt.-% of vinyl esters; and
e7) 0 to 10 wt.-% of ethylenically unsaturated silanes,
the weight percentages being based on the total monomers in the mixture.

### Claim 6 (depends on 1)

A method for coating or impregnating a substrate, comprising contacting the substrate with the polymer latex according to claim 1.

### Claim 7 (depends on 1)

The polymer latex composition according to claim 1, wherein the oxirane functional compound is selected from
i) a latex polymer;
ii) monomeric or oligomeric compounds comprising at least two oxirane functional groups; and
iii) monomeric compounds, oligomeric or polymeric compounds that are not prepared by free-radical addition polymerization bearing at least one oxirane group and a functional group different from an oxirane group, the functional groups different from an oxirane group on different molecules of compound iii) are capable of reacting with each other.

### Claim 8 (depends on 1)

The polymer latex composition according to claim 1, wherein the carboxylic acid functional latex polymer and the oxirane functional compound are present in relative amounts to provide a molar ratio of oxirane groups to carboxylic acid groups from 0.1 to 2.

### Claim 9 (depends on 1)

A compounded latex composition suitable for the production of dip-molded articles comprising the polymer latex composition according to claim 1 and adjuvants selected from sulfur vulcanization agents, accelerators for sulfur vulcanization, crosslinkers, polyvalent cations and combinations thereof.

### Claim 10 (depends on 9)

The compounded latex composition according to claim 9, comprising 0 to 2.8 wt.-% of sulfur vulcanization agents and 0.5 wt.-% to 2.5 wt.-% of ZnO the weight percentages being based on solid latex polymer.

### Claim 11 (depends on 9)

A method for making dip-molded articles by
a) providing a compounded latex composition of claim 9;
b) immersing a mold having the desired shape of the final article in a coagulant bath comprising a solution of a metal salt;
c) removing the mold from the coagulant bath and optionally drying the mold;
d) immersing the mold as treated in step b) and c) in the compounded latex composition of step a);
e) coagulating a latex film on the surface of the mold;
f) removing the latex-coated mold from the compounded latex composition and optionally immersing the latex-coated mold in a water bath;
g) optionally drying the latex-coated mold;
h) heat treating the latex-coated mold obtained from step e) or f) at a temperature of 40° C. to 180° C.; and
i) removing the latex article from the mold.

### Claim 12 (depends on 11)

The method of claim 11, wherein after step a) and prior to step d) the compounded latex composition is matured for at least 3 hrs.