# US 12,415,219 B2 · Stable dispersions of monocrystalline nanometric silver particles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 12,415,219 B2
- Document ID: US12415219B2
- Status: Granted
- Kind: B2
- Application number: 18/637,403
- Filed: 2024-04-16
- Published: 2024-12-12
- Granted: 2025-09-16
- Earliest claimed: 2010-12-06
- Assignees: P.V. Nano Cell Ltd.
- Applicants: P.V. Nano Cell Ltd.
- Inventors: Fernando De La Vega; Ganit Shter Bar Joshua; Semyon Melamed; Reuven Geva; Moshe Link
- Web page: https://patentgrep.com/patent/US12415219B2

## CPC

- B22F 9/24: starting from liquid metal compounds, e.g. solutions
- B22F 1/0545: Dispersions or suspensions of nanosized particles
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- C09D 11/52: Electrically conductive inks
- G03C 1/8255: {Silver or silver compounds therefor}
- H01B 1/22: the conductive material comprising metals or alloys
- B22F 2009/245: {Reduction reaction in an Ionic Liquid [IL]}
- B22F 2301/255: Silver or gold
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- G03C: PHOTOSENSITIVE MATERIALS FOR PHOTOGRAPHIC PURPOSES (for photomechanical purposes G03F); PHOTOGRAPHIC PROCESSES, e.g. CINE, X-RAY, COLOUR, STEREO-PHOTOGRAPHIC PROCESSES; AUXILIARY PROCESSES IN PHOTOGRAPHY (photographic processes characterised by the use or manipulation of apparatus classifiable per se in subclass G03B, see G03B; photomechanical production of textured or patterned surfaces G03F; electrophotography, magnetography G03G)
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})

## Abstract

A concentrated dispersion of nanometric silver particles, and a method of producing the dispersion, the dispersion including a first solvent; a plurality of nanometric silver particles, in which a majority are single-crystal silver particles, the plurality of nanometric silver particles having an average secondary particle size (d50) within a range of 30 to 300 nanometers, the particles disposed within the solvent; and at least one dispersant; wherein a concentration of the silver particles within the dispersion is within a range of 30% to 75%, by weight, and wherein a concentration of the dispersant is within a range of 0.2% to 30% of the concentration of the silver particles, by weight.

## Claims

### Claim 1

A concentrated dispersion of nanometric silver particles, the dispersion comprising:
(a) a first solvent;
(b) nanometric silver particles, in which a majority of said nanometric silver particles are single-crystal silver particles having an average secondary particle size (d50) within a range of 30 to 200 nanometers, said nanometric silver particles disposed within said first solvent, wherein at least 50% of a group of at least 10 randomly-selected electron back scattered diffraction (EBSD) scans produce a substantially perfect match for a single crystal; and
(c) at least one dispersant,
wherein a concentration of said nanometric silver particles within the concentrated dispersion is within a range of 30% to 75%, by weight,
and wherein a concentration of said dispersant within the dispersion is within a range of 0.2% to 30% of said concentration of said nanometric silver particles, by weight.

### Claim 2 (depends on 1)

The dispersion of claim 1, wherein said concentration of said dispersant within the dispersion is at most 20%.

### Claim 3 (depends on 1)

The dispersion of claim 1, wherein said average secondary particle size is at least 40 nanometers.

### Claim 4 (depends on 1)

The dispersion of claim 1, wherein at least 60% of said nanometric silver particles are said single-crystal silver particles.

### Claim 5 (depends on 1)

The dispersion of claim 1, wherein said average secondary particle size is at most 150 nanometers.

### Claim 6 (depends on 1)

The dispersion of claim 1, wherein said at least one dispersant is selected from the group of dispersants consisting of a polyvinylpyrrolidone (PVP), gum arabic, polyvinyl alcohol (PVA), polyacrylic acid (PAA), polyallylamine (PAAm), polysodium styrene sulfonate (PSS), 3-(aminopropyl) trimethoxysilane (APS), a fatty acid, lauryl amine, cetyltrimethylammonium bromide (CTAB), and tetraoctylammonium bromide (TOAB).

### Claim 7 (depends on 6)

The dispersion of claim 6, wherein said dispersant includes PVP, and wherein an average molecular weight of said PVP is within a range of 10,000 gram/mole to 1,600,000 gram/mole.

### Claim 8 (depends on 1)

The dispersion of claim 1, wherein said first solvent includes water.

### Claim 9 (depends on 1)

The dispersion of claim 1, wherein said first solvent includes an alcohol.

### Claim 10

A method for producing a dispersion of nanometric silver particles, the method comprising the steps of:
(a) reacting at least one soluble silver compound with an alkali metal hydroxide in an aqueous medium, in a presence of a first dispersant, to produce silver oxide solids having an average secondary particle size below 1200 nanometers;
(b) reacting said silver oxide solids with at least one reducing agent in an aqueous medium, in a presence of a second dispersant, to produce a first dispersion of silver particles, the silver particles having an average secondary particle size below 300 nanometers; and
(c) removing at least a portion of said aqueous medium of step (b) from the silver particles to produce the dispersion of the nanometric silver particles;
wherein said alkali metal hydroxide and said at least one soluble silver compound react in a stoichiometric ratio of said alkali metal hydroxide to said at least one soluble silver compound, and wherein quantities of said alkali metal hydroxide and said at least one soluble silver compound are added to said aqueous medium in a particular ratio that is at most 0.98 moles of said alkali metal hydroxide to one mole of said at least one soluble silver compound;
wherein a concentration of said silver particles within said first dispersion is within a range of 0.5% to 5%, by weight of said first dispersion;
wherein more than 50% by weight of the nanometric silver particles are single-crystal silver particles;
and wherein an excess of said second dispersant is removed in step (c).

### Claim 11 (depends on 10)

The method of claim 10, further comprising the step of further concentrating the silver particles within the dispersion of the nanometric silver particles produced in step (c), to form a second dispersion.

### Claim 12 (depends on 11)

The method of claim 11, wherein a concentration of the silver particles within said second dispersion is at least 10%, and less than 75%, by weight.

### Claim 13 (depends on 10)

The method of claim 10, wherein step (c) includes washing and concentrating the silver particles, whereby the aqueous medium is partially removed from the silver particles, to form a concentrate, the concentrate containing most of the silver particles from step (b).

### Claim 14 (depends on 13)

The method of claim 13, further comprising the steps of replacing most of said aqueous medium by at least one volatile organic solvent, and replacing most of said volatile organic solvent by at least one additional organic solvent.

### Claim 15 (depends on 10)

The method of claim 10, wherein a concentration of said nanometric silver particles within the dispersion of nanometric silver particles is within a range of 30% to 75%, by weight.

### Claim 16 (depends on 10)

The method of claim 10, wherein a concentration of said first and second dispersants within the dispersion of nanometric silver particles is within a range of 0.2% to 30% of said concentration of said nanometric silver particles, by weight.

### Claim 17 (depends on 10)

The method of claim 10, wherein a concentration of said first and second dispersants is at least 0.2%, by weight, of said concentration of said silver particles and is at most 10% of said concentration of said particles, by weight.

### Claim 18 (depends on 10)

The method of claim 10, wherein, subsequent to step (c), the dispersion of the nanometric silver particles is aged for 6 months, and wherein more than 50% by weight of the nanometric silver particles remain single-crystal silver particles.

### Claim 19 (depends on 10)

The method of claim 10, wherein, with respect to said nanometric silver particles, at least 50% of a group of at least 10 randomly-selected electron back scattered diffraction (EBSD) scans produce a substantially perfect match for a single crystal.