MySx/ZSH mixture as sulfidizing agent
AssigneeNouryon Chemicals International B.V.
InventorsMatthias Folchnandt, Olaf Klobes, Ulises Picardi, Rodrigo M. Giménez, Leandro Prats
Life of this patent
Estimating the term…
Abstract
The disclosure is directed to a sulfidizing agent obtainable by mixing MySx and ZSH in a weight ratio of from about 90:10 to about 10:90, wherein M is chosen from Li+, Na+, K+, Rb+, Cs+, NH4+, Mg2+ and Ca2+, y is about 1 or about 2, x is from about 1.1 to about 5, and Z is independently chosen from Li+, Na+, K+, Rb+, Cs+ and NH4+, and a process for using the sulfidizing agent in the recovery of one or more metal ores and/or polymetallic minerals from gangue.
Claims18
A process for recovering one or more metal ores and/or polymetallic minerals from gangue, said process comprising:
- (i) treating the one or more metal ores and/or polymetallic minerals with a sulfidizing agent;
- and
- (ii) separating the treated metal ores and/or polymetallic minerals using a sulfide floatation process;
- wherein the sulfidizing agent is obtained by mixing MySx and ZSH in a weight ratio of from about 90:10 to about 10:90, wherein M is chosen from Li+, Na+, K+, Rb+, Cs+, NH4+, Mg2+ and Ca2+, y is about 1 or about 2, x is from about 2.1 to about 5, and Z is independently chosen from Li+, Na+, K+, Rb+, Cs+ and NH4+;
- wherein the treatment in (i) is performed by adding a first portion of sulfidizing agent to the one or more metal ores and/or polymetallic minerals in a rougher floatation stage of the sulfide floatation process and adding a further portion of sulfidizing agent to the one of metal ores and/or polymetallic minerals in at least one cleaning stage of the sulfide floatation process;
- and
- wherein the sulfidizing agent is added to the rougher floatation stage in an amount of from about 10 to about 70 g/ton and to the at least one cleaning stage in an amount of from about 3 to about 15 g/ton, based on a dose of grams of agent per ton of dry ore/dry mineral.