Abstract
An insulating fill material composition for use in outerwear, sleeping bags, bedding, and the like includes 40.0 to 85.0 wt % alpaca fibers, 10.0 to 20.0 wt % bicomponent fibers, and 5.0 to 40.0 wt % polyester fibers. The alpaca fibers have a length of 40.0 to 70.0 mm. The bicomponent fibers have a length of 40.0 mm to 60.0 mm and a linear mass density of 0.11 to 0.33 mg/m. The polyester fibers have a length of 40.0 mm to 60.0 mm and a linear mass density of 0.22 to 0.44 mg/m. Blending, combing, carding, and lapping of the alpaca fibers, the bicomponent fibers, and the polyester fibers forms a matte, which when needled and heated forms a batting having a weight of 50.0 to 400.0 g/m2.
Claims3
A method of preparing an insulating fill material composition comprising the steps of:
- providing insulating fill material components comprising:
- 40.0 to 85.0 wt % alpaca fibers having a length of 40.0 to 70.0 mm,
- 10.0 to 20.0 wt % bicomponent fibers having a length of 40.0 mm to 60.0 mm and a linear mass density of 0.11 to 0.33 mg/m, and
- 5.0 to 40.0 wt % polyester fibers having a length of 40.0 mm to 60.0 mm and a linear mass density of 0.22 to 0.44 mg/m;
- blending and combing the alpaca fibers, the bicomponent fibers, and the polyester fibers to form a substantially homogeneous mixture;
- carding the substantially homogeneous mixture to substantially align the alpaca fibers, the bicomponent fibers, and the polyester fibers to create a web of fibers;
- lapping the web of fibers to form a matte;
- needling the matte to entangle the alpaca fibers, the bicomponent fibers, and the polyester fibers;
- heating the matte to form a batting;
- providing a solution of an antistatic compound;
- and
- spraying the solution of the antistatic compound onto the alpaca fibers, the bicomponent fibers, and the polyester fibers during the blending and combing step, onto the substantially homogeneous mixture during the carding step, and onto the web of fibers during the lapping step.
A method of preparing an insulating fill material composition comprising the steps of:
- providing insulating fill material components comprising:
- 40.0 to 85.0 wt % alpaca fibers having a length of 40.0 to 70.0 mm,
- 10.0 to 20.0 wt % bicomponent fibers having a length of 40.0 mm to 60.0 mm and a linear mass density of 0.11 to 0.33 mg/m, and
- 5.0 to 40.0 wt % polyester fibers having a length of 40.0 mm to 60.0 mm and a linear mass density of 0.22 to 0.44 mg/m;
- blending and combing the alpaca fibers, the bicomponent fibers, and the polyester fibers to form a substantially homogeneous mixture;
- carding the substantially homogeneous mixture to substantially align the alpaca fibers, the bicomponent fibers, and the polyester fibers to create a web of fibers;
- lapping the web of fibers to form a matte;
- needling the matte to entangle the alpaca fibers, the bicomponent fibers, and the polyester fibers;
- heating the matte to form a batting;
- providing glycidyl methacrylate or a solution thereof;
- and
- spraying the glycidyl methacrylate or the solution thereof onto each opposed face of the matte prior to and/or during heating of the matte.