Abstract
A pressure sensitive adhesive particle includes a styrene resin; and a (meth)acrylate resin, wherein the (meth)acrylate resin contains two kinds of (meth)acrylates as a polymerization component in which the weight proportion of the (meth)acrylate to the total polymerization components is 90% by weight or more, and has two glass transition points in which a difference between the lowest glass transition temperature and the highest glass transition temperature is 30° C. or higher.
Claims12
A pressure sensitive adhesive particle comprising:
- a styrene resin;
- and
- a (meth)acrylate resin,
- wherein the styrene resin is derived from styrene resin polymerization components, the styrene resin polymerization components including styrene and at least one selected from the group consisting of 2-ethyl hexyl acrylate and n-butyl acrylate,
- wherein the (meth)acrylate resin is derived from alkyl (meth)acrylate polymerization components, the alkyl (meth)acrylate polymerization components including 2-ethyl hexyl acrylate and n-butyl acrylate,
- a weight proportion of the alkyl (meth)acrylate polymerization components to a total polymerization components of the (meth)acrylate resin is 90% by weight or more,
- the pressure sensitive adhesive has two glass transition points,
- a difference between a lowest glass transition temperature and a highest glass transition temperature of the pressure sensitive adhesive is 30° C. or higher,
- a weight ratio among the 2-ethyl hexyl acrylate and n-butyl acrylate of the alkyl (meth)acrylate polymerization components of the (meth)acrylate resin is from 80:20 to 20:80,
- the pressure sensitive adhesive particle includes:
- a core portion that contains the styrene resin and the (meth)acrylate resin;
- and
- a shell layer that covers the core portion and contains the styrene resin,
- a glass transition temperature of the (meth)acrylate resin is −10° C. or lower,
- the core portion comprises:
- a sea phase that contains the styrene resin;
- and
- an island phase that contains the (meth)acrylate resin dispersed in the sea phase, and
- an average diameter of the island phases is from 200 nm to 500 nm.