A process of extraction, quantification and recovery of additives in polypropylene comprising the following stages:
- stage 1) washing a plastic material (A);
- stage 2) grinding the plastic material (A) to a particle size from 10 to 500 microns;
- stage 3) carrying out an extraction process where the plastic material (A) of stage 2) is transferred to a first column and thereafter the plastic material (A) passes through a second column, a third column and a fourth column respectively for successive extractions with a first solvent, a second solvent, a third solvent and a fourth solvent, respectively, to obtain a first, second, third and fourth solvent with additives;
- stage 4) carrying out packed column extraction, wherein the first, second, third and fourth solvent with the additives obtained from each extraction in the first, second, third and fourth columns from stage 3) passes through a first packed column a second packed column, a third packed column and a fourth packed column respectively to obtain a first additive, a second additive, a third additive and fourth additive;
- stage 5) crystallizing the additives obtained from each extraction stage in the first, second, third and fourth packed columns respectively from stage 4);
- and
- stage 6) quantifying the crystallized additives obtained from stage 5);
- wherein a residue material without additives is subjected to a subsequent pyrolysis process,
- wherein in stage 4), the first, second, third and fourth
- packed columns each comprises a different packing, and
- wherein
- the first packed column contains from 85% to 95% of a modified styrene-divinylbenzene polymer (Strata X-33), from 7.5% to 2.5% of activated charcoal and from 2.5% to 7.5% of silanized glass wool;
- the second packed column contains from 80% to 90% of a modified styrene-divinylbenzene polymer (Strata X-33), from 7.5% to 15% of activated charcoal and from 2.5% to 5% of silanized glass wool;
- the third packed column contains from 70% to 90% of a modified styrene-divinylbenzene polymer (Strata X-33), from 5% to 15% of activated charcoal and from 5% to 15% of silanized glass wool;
- and
- the fourth packed column contains from 70% to 90% of a modified styrene-divinylbenzene polymer (Strata X-33), from 5% to 15% of activated charcoal and from 5% to 15% of silanized glass wool.