US 12,319,630 B2Granted
Phlego cement from a new earth-inspired clinker
AssigneeThe Board of Trustees of the Leland Stanford Junior University
InventorTiziana Vanorio
Life of this patent
Estimating the term…
Abstract
Improved cement for concrete is provided having reduced carbon footprint and improved mechanical properties. A limestone-free process of making the clinker provides a 70% reduction of carbon footprint vs. conventional manufacture of Portland cement. Curing the resulting cement in a temperature range from 80° C. to 100° C. advantageously enhances growth of fibrous minerals in the concrete.
Claims3
A method of making a clinker for use in cement production, the method comprising:
- providing raw meal including silica, aluminum oxide, alkali oxides, calcium oxide and sulfur oxide;
- wherein a weight fraction of silica in the raw meal is between 40% and 60%;
- wherein a weight fraction of the aluminum oxide in the raw meal is between 10% and 25%;
- wherein a weight fraction of the alkali metal oxides in the raw meal is between 5% and 15%;
- wherein a weight fraction of the calcium oxide in the raw meal is between 5% and 15%;
- wherein a weight fraction of the sulfur oxide in the raw meal is between 0.5% and 2%;
- wherein a weight fraction of carbon-containing chemical species in the raw meal is less than 1%;
- firing the raw meal to provide the clinker.
5 more elements