Method for producing a rubber-plastic composite
AssigneeContinental Reifen Deutschland GmbH
InventorsKonstantin Efimov, Anna-Lena Dreier, Klaus Hülsmann, Andreas Pawlik, Marco Kormann, Maximilian Drexler
Life of this patent
Estimating the term…
Loading patent…
AssigneeContinental Reifen Deutschland GmbH
InventorsKonstantin Efimov, Anna-Lena Dreier, Klaus Hülsmann, Andreas Pawlik, Marco Kormann, Maximilian Drexler
Estimating the term…
A method for producing a rubber-plastic composite, including the steps of (a) shaping an unvulcanized elastomer, (b) partially vulcanizing the shaped elastomer at a temperature of at least 140° C. up to a degree of vulcanization in the range from 10% to 40%, (c) cooling the partially vulcanized elastomer to a temperature of less than 100° C. within less than 20 minutes, (d) overmolding the partially vulcanized elastomer with a plastic, and (e) heat treating the partially vulcanized elastomer overmolded with a plastic at a temperature in the range from 100° C. to 170° C. for a duration of from 5 minutes to 5 hours to complete the vulcanization and form a rubber-plastic composite. The method further relates to a rubber-plastic composite obtainable by the method according to the invention and also to a shoe comprising the rubber-plastic composite obtainable by the method according to the invention.
A method for producing a rubber-plastic composite, comprising the following steps:
A method for producing a rubber-plastic composite, comprising the following steps:
Dependencies are inferred from the claim text.