Absorbent article comprising a lotion resistant polymeric filler composition
AssigneeThe Procter & Gamble Company
InventorsRobert Haines Turner, John Andrew Strasemeier
Life of this patent
Estimating the term…
Abstract
Described herein is an absorbent article including (a) an absorbent core, a first nonwoven material, a second nonwoven material, and a bond area; and (b) a polymeric filler composition disposed within the bond area. The polymeric filler composition has less than 5% of a tackifier. The polymeric filler composition is chosen from a propylene butene copolymer, a polypropylene homopolymer, a propylene ethylene copolymer, and mixtures thereof. The polymeric filler composition has a Tensile Strength at Yield of from about 0.5 MPa to about 10 MPa.
Claims12
An absorbent article comprising:
- a) an absorbent core, a first nonwoven material, a second nonwoven material, and a bond area joining a portion of the first nonwoven material and a portion of the second nonwoven material;
- and
- b) a polymeric filler composition disposed within the bond area;
- wherein the polymeric filler composition comprises less than 5% of a tackifier by weight of the polymeric filler composition;
- wherein the polymeric filler composition is selected from the group consisting of a propylene butene copolymer, a polypropylene homopolymer, a propylene ethylene copolymer, and mixtures thereof;
- wherein the polymeric filler composition has a Tensile Strength at Yield of from about 0.5 MPa to about 10 MPa according to the Tensile Strength Test Method described herein.
An absorbent article comprising:
- a) an absorbent core, a first nonwoven material, a second nonwoven material, and a bond area joining a portion of the first nonwoven material and a portion of the second nonwoven material;
- and
- b) a polymeric filler composition disposed within the bond area;
- wherein the polymeric filler composition comprises at least 98% of a polymer selected from the group consisting of a propylene butene copolymer, a polypropylene homopolymer, a propylene ethylene copolymer, and mixtures thereof;
- wherein the polymeric filler composition comprises less than 5% of a tackifier by weight of the polymeric filler composition;
- wherein the polymeric filler composition has a Tensile Strength at Yield of from about 0.5 MPa to about 10 MPa according to the Tensile Strength Test Method described herein.
Dependencies are inferred from the claim text.