# US 12,225,743 B2 · Long-acting and stable perovskite solar cell and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 12,225,743 B2
- Document ID: US12225743B2
- Status: Granted
- Kind: B2
- Application number: 18/818,668
- Filed: 2024-08-29
- Published: 2024-12-19
- Granted: 2025-02-11
- Earliest claimed: 2023-02-28
- Assignees: Nanjing University of Posts and Telecommunications
- Applicants: Nanjing University of Posts & Telecommunications
- Inventors: Ligang Xu; Wenxuan Lv; Runfeng Chen; Wei Huang
- Web page: https://patentgrep.com/patent/US12225743B2

## CPC

- H10K 30/88: Passivation; Containers; Encapsulations
- H10K 30/10: comprising heterojunctions between organic semiconductors and inorganic semiconductors
- H10K 30/151: {the wide bandgap semiconductor comprising titanium oxide, e.g. TiO2}
- H10K 30/40: comprising a p-i-n structure, e.g. having a perovskite absorber between p-type and n-type charge transport layers
- H10K 30/50: Photovoltaic [PV] devices
- H10K 71/15: characterised by the solvent used
- H10K 71/40: Thermal treatment, e.g. annealing in the presence of a solvent vapour
- H10K 85/50: Organic perovskites; Hybrid organic-inorganic perovskites [HOIP], e.g. CH3NH3PbI3
- Y02E 10/549: Organic PV cells
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A long-lasting and stable perovskite solar cell utilizes fluorine-containing inorganic ammonium salts to form ion exchange with perovskite to construct a perovskite light-absorbing layer to protect the perovskite, greatly improving stability of the perovskite solar cell. The perovskite solar cell can maintain 94% and 81% of its initial efficiency after being placed in a nitrogen-filled glove box and humid air for 14,016 hours and 2,500 hours, respectively, and can still maintain 83% of its initial efficiency after performed by heat aging at 85° C. for 1,248 hours, reaching a world-class level. A preparation method of the perovskite solar cell is simple, materials used to prepare the perovskite solar cell are inexpensive, and the stability of an obtained device is significantly improved under various conditions.

## Claims

### Claim 1

A perovskite solar cell, characterized in that a structure of the perovskite solar cell comprises: a substrate, an anode layer, a hole-transporting layer, a perovskite multi-protective layer, a composite electron-transporting layer, a hole blocking layer, and a metal cathode layer that are arranged sequentially from bottom to top of the structure of the perovskite solar cell;
wherein the perovskite multi-protective layer comprises: a perovskite light-absorbing layer and a multifunctional protection layer, the perovskite multi-protective layer is configured to improve a stability of the perovskite solar cell through triple protection, and the triple protection comprises: an ion exchange reaction, a hydrophobic effect and hydrogen bonding based on raw materials of the perovskite solar cell, and passivation of perovskite defects; and
wherein a preparation method of the perovskite solar cell comprises the following steps:
preparing the anode layer on the substrate by using transparent glass as the substrate, and spin-coating a poly[bis(4-phenyl)(2,4,6-trimethylphenyl)amine] (PTAA) solution on the anode layer to obtain the hole-transporting layer;
spin-coating a perovskite precursor solution on the hole-transporting layer by using a one-step anti-solvent method;
wherein the perovskite precursor solution is prepared by dissolving formamidinium iodide (FAI), methylammonium bromide (MABr), lead(II) bromide (PbBr2), and lead(II) iodide (PbI2) in a mixed solvent of N,N-dimethylformamide (DMF) and dimethyl sulfoxide (DMSO) with a volume ratio of the DMF to the DMSO being 4:1 to obtain a first mixed solution, then dissolving cesium iodide (CsI) in DMSO to obtain a second mixed solution, and mixing the first mixed solution and the second mixed solution before spin-coating the perovskite precursor solution; and a speed of spin-coating the perovskite precursor solution is in a range of 5,000 revolutions per minute (rpm) to 10,000 rpm, and a time for spin-coating the perovskite precursor solution is 55 seconds (s);
dropwise adding an anti-solvent of ethyl acetate (EA) containing ammonium hexafluorophosphate (NH4PF6) during spin-coating the perovskite precursor solution, wherein a concentration of the NH4PF6 in the anti-solvent of EA containing NH4PF6 is 1 milligram per milliliter (mg/mL), a time for dropwise adding the anti-solvent of EA containing the NH4PF6 is 15 s before finishing spin-coating the perovskite precursor solution, and an addition amount of the anti-solvent of EA is 150 microliters (μL);
placing the hole-transporting layer coated with the perovskite precursor solution on a heating stage for an annealing reaction after finishing spin-coating the perovskite precursor solution, and obtaining the perovskite multi-protective layer after the annealing reaction is finished;
wherein a lower portion of the perovskite multi-protective layer is a perovskite crystal with a composition of (Cs0.05FA0.81MA0.14)Pb(Br0.14I0.86)3 and an upper portion of the perovskite multi-protective layer is an ion-exchanged perovskite crystal with a composition of (Cs0.05FA0.81MA0.14)Pb(Br0.14I0.86-x(PF6)x)3 that together constitute the perovskite light-absorbing layer of the perovskite multi-protective layer, and a top surface of the perovskite multi-protective layer is the multifunctional protection layer made from the NH4PF6;
spin-coating a [6,6]-phenyl C61 butyric acid methyl ester (PC61BM) solution on the multifunctional protection layer to obtain a PC61BM layer, and then depositing fullerene (C60) on the PC61BM layer to construct the composite electron-transporting layer; and
wherein a lower layer of the composite electron-transporting layer is the PC61BM layer, and an upper layer of the composite electron-transporting layer is the C60;
evaporating lithium fluoride (LiF) on the composite electron-transporting layer as the hole blocking layer, and then evaporating a metal material on the hole blocking layer to form the metal cathode layer, thereby obtaining the perovskite solar cell.

### Claim 2 (depends on 1)

The perovskite solar cell as claimed in claim 1, wherein a reaction temperature for the annealing reaction is in a range of 70 degrees Celsius (° C.) to 120° C., and a reaction time for the annealing reaction is in a range of 5 min to 20 min.

### Claim 3 (depends on 1)

The perovskite solar cell as claimed in claim 1, wherein the perovskite solar cell is capable of maintaining long-term stability under various conditions, maintaining 94% and 81% of an initial efficiency of the perovskite solar cell after being placed in a nitrogen-filled glove box and humid air for 14,016 hours (h) and 2,500 h, respectively, and maintaining 83% of the initial efficiency of the perovskite solar cell after performed by heat aging at 85° C. for 1,248 h.