# US 12,214,393 B2 · Magnesium or magnesium alloy having ultra-high formability at room temperature and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 12,214,393 B2
- Document ID: US12214393B2
- Status: Granted
- Kind: B2
- Application number: 16/649,867
- Filed: 2018-09-21
- Published: 2020-08-27
- Granted: 2025-02-04
- Earliest claimed: 2017-09-25
- Assignees: Baoshan Iron & Steel Co., Ltd.; China Baowu Steel Group Corporation Limited
- Applicants: Baoshan Iron & Steel Co., Ltd.; China Baowu Steel Group Corporation Limited
- Inventors: Jianfeng Nie; Zhuoran Zeng; Shiwei Xu; Nick Birbilis; Christopher H. J. Davies; Weineng Tang
- Web page: https://patentgrep.com/patent/US12214393B2

## CPC

- B21C 23/002: {Extruding materials of special alloys so far as the composition of the alloy requires or permits special extruding methods of sequences}
- C22C 23/00: Alloys based on magnesium
- C22F 1/06: of magnesium or alloys based thereon
- B21C: MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES, PROFILES OR LIKE SEMI-MANUFACTURED PRODUCTS OTHERWISE THAN BY ROLLING; AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKING WITHOUT ESSENTIALLY REMOVING MATERIAL
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

The present invention provides magnesium or magnesium alloys having high formability at room temperature, the magnesium or magnesium alloys having a grain size ≤2 microns. The present invention also provides a method for manufacturing the magnesium or magnesium alloys having high formability at room temperature. The magnesium or magnesium alloys having high formability at room temperature are prepared by simple processing means. The present invention overcomes a problem of poor formability at room temperature.

## Claims

### Claim 1

A manufacturing method for manufacturing a magnesium alloy extrusion product, extruding a magnesium alloy raw material ingot at a temperature of 20-80° C. and an extrusion ratio of 10:1 to 100:1 to obtain the magnesium alloy extrusion product,
wherein the magnesium alloy extrusion product consists of magnesium, silver, and strontium and has ultra-high room temperature formability and a grain size of ≤2 μm.

### Claim 2 (depends on 1)

The manufacturing method according to claim 1, wherein the magnesium alloy raw matermial ingot is extruded at an extrusion push rod speed of 0.05 mm/s-50 mm/s.

### Claim 3 (depends on 1)

The manufacturing method according to claim 1, wherein the magnesium alloy extrusion product has a grain size of ≤1 μm.

### Claim 4 (depends on 1)

The manufacturing method according to claim 1, wherein the magnesium alloy extrusion product is further rolled at 20-100° C. to form a magnesium alloy plate consisting of magnesium, silver, and strontium.

### Claim 5 (depends on 4)

The manufacturing method according to claim 4, wherein the magnesium alloy plate has a thickness of 0.3 mm to 4 mm or 0.04 to 0.03 mm.

### Claim 6 (depends on 1)

The manufacturing method according to claim 1, wherein a total mass percentage of silver and strontium is ≤1.5%.