Method of restoring alloy depletion in an airfoil around cooling holes
AssigneeRtx Corporation
InventorsBrian Richard Craig, Michael J. Minor, Randall D. Kelton, Arka Ray, Xuan Liu
Life of this patent
Estimating the term…
Loading patent…
AssigneeRtx Corporation
InventorsBrian Richard Craig, Michael J. Minor, Randall D. Kelton, Arka Ray, Xuan Liu
Estimating the term…
A method of reducing depletion of elements from an airfoil includes disposing a bond coating on the airfoil, where the airfoil comprises cooling channels. The airfoil includes a material that has an initial composition. A cooling hole is machined in the airfoil to contact the cooling channels such that a fluid travelling in the cooling channel may be discharged via the cooling hole. The machining of the cooling hole results in a formation of a depleted region around the cooling hole. The depleted region is depleted of a portion of the initial composition of the airfoil. A top coat is disposed on the bond coat. The airfoil is subjected to a heat treatment at a temperature effective to promote diffusion of elements from a non-depleted region to the depleted region around the cooling hole.
A method of reducing depletion of elements from an airfoil comprising:
Dependencies are inferred from the claim text.