# US 12,180,391 B2 · Preinstalled sealant for prefab components

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 12,180,391 B2
- Document ID: US12180391B2
- Status: Granted
- Kind: B2
- Application number: 17/591,886
- Filed: 2022-02-03
- Published: 2022-08-04
- Granted: 2024-12-31
- Earliest claimed: 2021-02-04
- Assignees: UT-Battelle, LLC
- Applicants: UT-Battelle, LLC
- Inventors: Diana Hun; Pengfei Cao; Xiao Zhao; Zoriana Demchuk; Jiancheng Luo; Tomonori Saito
- Web page: https://patentgrep.com/patent/US12180391B2

## CPC

- C09J 133/12: Homopolymers or copolymers of methyl methacrylate
- C09J 5/00: Adhesive processes in general; Adhesive processes not provided for elsewhere, e.g. relating to primers
- C09J 11/08: Macromolecular additives
- C09J 133/08: Homopolymers or copolymers of acrylic acid esters
- C09J 2203/346: for building applications e.g. wrap foil
- C09J 2301/412: presence of microspheres
- C09J 2433/00: Presence of (meth)acrylic polymer
- C09J 2463/00: Presence of epoxy resin
- C09J 2475/00: Presence of polyurethane
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)

## Abstract

A joint sealing system for prefabricated building components is provided. The joint sealing system includes a first component including a first surface, and a second component including a second surface that is mateable with the first surface. The first and second surfaces define a joint. A sealant composition is disposed on one of the first surface or the second surface. Pressure exerted when the second surface is mated with the first surface triggers curing of the sealant composition to join the first and second components and to seal the joint between the first and second components. A method of joining and sealing two prefabricated building components is also provided.

## Claims

### Claim 1

A joint sealing system for prefabricated building components comprising:
a first component including a first surface;
a second component including a second surface that is mateable with the first surface, said first and second surfaces defining a joint; and
a sealant composition disposed on one of the first surface or the second surface, the sealant composition comprising:
a first component including a curing agent and a polymer matrix, the curing agent including one or more of diamine-type curing agents and diol-type curing agents; and
a second component that includes a microcapsule having a resin encapsulated inside a shell, the resin including one or more of epoxy-based resins, acrylic-based resins, aliphatic isocyanate-based resins, and aromatic isocyanate-based resins, and the microcapsule being dispersed in the first component;
wherein breaking of the microcapsule shell by an applied force allows the curing agent to react with the resin to cure the sealant composition;
wherein pressure exerted when the second surface is mated with the first surface triggers curing of the sealant composition to join the first and second components and to seal the joint between the first and second components.

### Claim 2 (depends on 1)

The joint sealing system of claim 1, wherein the first surface includes a male connector and the second surface includes a female connector.

### Claim 3 (depends on 2)

The joint sealing system of claim 2, wherein the sealant composition is either: (i) disposed in the female connector; or (ii) disposed adjacent the male connector.

### Claim 4 (depends on 1)

The joint sealing system of claim 1, wherein the joint is one selected from (i) a tongue-and-groove joint; or (ii) a butt joint.

### Claim 5 (depends on 1)

The joint sealing system of claim 1, wherein the sealant composition is a preinstalled sealant that is disposed on the first surface or the second surface during manufacturing of the first or second component.

### Claim 6 (depends on 1)

The joint sealing system of claim 1, wherein the polymer matrix is a healable polymer that is a copolymer including an acrylate monomer unit having a low glass transition temperature (Tg) and a methacrylate monomer unit having a high glass transition temperature (Tg).

### Claim 7 (depends on 6)

The joint sealing system of claim 6, wherein the healable polymer includes one or both of butyl acrylate (BA) and 2-ethylhexyl acrylate (2-EHA) combined with methyl methacrylate (MMA) in a ratio of between 95:5 and 50:50.

### Claim 8 (depends on 1)

The joint sealing system of claim 1, wherein the curing agent is one or more selected from a PPG/PEG-diamine, a PPG-di (secondary amine), a PPG/PEG-triamine, a polyethyleneimine (PEI), and a PPG/PEG-diol.

### Claim 9 (depends on 8)

The joint sealing system of claim 8, wherein the curing agent is (i) a combination of a PPG/PEG-triamine and polyethyleneimine (PEI) wherein the amount of PEI is between 0 and 40% by weight; (ii) a combination of a PPG/PEG-diamine and a PPG/PEG-diol wherein the amount of PPG/PEG-diol is between 0 and 60% by weight; and (iii) a combination of a PPG-di (secondary amine) and a PPG/PEG-diol wherein the amount of PPG/PEG-diol is between 0 and 60% by weight.

### Claim 10 (depends on 1)

The joint sealing system of claim 1, wherein the resin is one or more selected from a bisphenol A epoxy, a novolac epoxy, an acrylated novolac epoxy, a bio-based epoxy, an aliphatic di-isocyanate, an aromatic di-isocyanate, a bio-based di-isocyanate, a diacrylate, and a triacrylate.

### Claim 11 (depends on 1)

The joint sealing system of claim 1, wherein the curing agent cures the resin in less than 8 hours and the resin is fully cured within 21 days at temperature between 2° and 100° F.

### Claim 12 (depends on 1)

The joint sealing system of claim 1, wherein the cured sealant composition has an adhesion strength of at least 15 pounds/inch.

### Claim 13 (depends on 1)

The joint sealing system of claim 1, wherein the microcapsule has a diameter in the range of 10 to 1000 μm and a shell thickness of between 1 and 50 μm.

### Claim 14

A method of joining and sealing two prefabricated building components, the method comprising:
providing a first component having a first surface;
providing a second component having a second surface that is mateable with the first surface, the first and second surfaces defining a joint;
disposing a sealant composition on one of the first surface or the second surface, the sealant composition comprising:
a first component including a curing agent and a polymer matrix, the curing agent including one or more of diamine-type curing agents and diol-type curing agents; and
a second component that includes a microcapsule having a resin encapsulated inside a shell, the resin including one or more of epoxy-based resins, acrylic-based resins, aliphatic isocyanate-based resins, and aromatic isocyanate-based resins, and the microcapsule being dispersed in the first component;
wherein breaking of the microcapsule shell by an applied force allows the curing agent to react with the resin to cure the sealant composition; and
joining the first component with the second component by mating the first surface with the second surface, whereby a force is applied to the sealant composition, causing the microcapsules to rupture such that the resin mixes with the curing agent and the sealant composition cures to seal the joint between the first component and the second component.

### Claim 15 (depends on 14)

The method of claim 14, wherein one or both of the components are fabricated at a location different than the location at which the components are assembled together, and the sealant composition is preinstalled by being disposed on one of the components at the said different location at which the components are fabricated.

### Claim 16

A joint sealing system for prefabricated building components comprising:
a first component including a first surface;
a second component including a second surface that is mateable with the first surface, said first and second surfaces defining a joint; and
a sealant composition disposed on one of the first surface or the second surface, the sealant composition comprising:
a first component including a curing agent and a polymer matrix, the polymer matrix being a healable polymer that is a copolymer including an acrylate monomer unit having a low glass transition temperature (Tg) and a methacrylate monomer unit having a high glass transition temperature (Tg); and
a second component that includes a microcapsule having a resin encapsulated inside a shell, the microcapsule being dispersed in the first component;
wherein breaking of the microcapsule shell by an applied force allows the curing agent to react with the resin to cure the sealant composition;
wherein pressure exerted when the second surface is mated with the first surface triggers curing of the sealant composition to join the first and second components and to seal the joint between the first and second components.

### Claim 17 (depends on 16)

The joint sealing system of claim 16, wherein the healable polymer includes one or both of butyl acrylate (BA) and 2-ethylhexyl acrylate (2-EHA) combined with methyl methacrylate (MMA) in a ratio of between 95:5 and 50:50.

### Claim 18 (depends on 16)

The joint sealing system of claim 16, wherein the curing agent cures the resin in less than 8 hours and the resin is fully cured within 21 days at temperature between 2° and 100° F.

### Claim 19 (depends on 16)

The joint sealing system of claim 16, wherein the cured sealant composition has an adhesion strength of at least 15 pounds/inch.

### Claim 20 (depends on 16)

The joint sealing system of claim 16, wherein the microcapsule has a diameter in the range of 10 to 1000 μm and a shell thickness of between 1 and 50 μm.