Infrared shielding film and infrared shielding material
AssigneeMitsubishi Materials Corporation
InventorsMiho Shoji, Satoko Higano, Hiroto Akaike
Life of this patent
Estimating the term…
Abstract
An infrared shielding film is an infrared shielding film including: an organic binder; and a plurality of tin-doped indium oxide particles (ITO particles) dispersed in the organic binder, in which the average center-to-center distance between adjacent particles of the ITO particles is in a range of 9 nm or more and 36 nm or less, the ratio of the average center-to-center distance between the adjacent particles to the average primary particle diameter of the ITO particles is in a range of 1.05 or more and 1.20 or less, and a roughness Ra of a film surface is in a range of 4 nm or more and 50 nm or less.
Claims3
An infrared shielding film comprising:
- an organic binder;
- and
- a plurality of tin-doped indium oxide particles dispersed in the organic binder,
- wherein the tin-doped indium oxide particles are produced using fatty acid salts of In and fatty acid salts of Sn, and surfaces of the tin-doped indium oxide particles are coated with an organic protective group derived from the fatty acid salts,
- the organic binder is one selected from the group consisting of (Z)-4-octenenitrile, (Z)-5-octenenitrile, (Z)-5-nonenenitrile, (Z)-6-undecenenitrile, (Z)-9-undecenenitrile, and (Z)-9-octadecenenitrile,
- an amount of the organic binder is in a range of 5 parts by mass or more and 30 parts by mass or less when an amount of the tin-doped indium oxide particles is 100 parts by mass,
- the tin-doped indium oxide particles are dispersed in a state of primary particles,
- an average center-to-center distance between adjacent particles of the tin-doped indium oxide particles is in a range of 9 nm or more and 36 nm or less,
- a ratio of the average center-to-center distance between the adjacent particles to an average primary particle diameter of the tin-doped indium oxide particles is in a range of 1.05 or more and 1.20 or less, and
- a roughness Ra of a film surface is in a range of 4 nm or more and 50 nm or less.