Abstract
Described herein is a method of adding one or more boronic acid functional compounds to a mineral ore to result in a treated mineral ore. Where the mineral ore is a bauxite ore, and the ore is subsequently processed according to the Bayer process to obtain alumina, adding a boronic acid functional compound to the bauxite ore or a Bayer product followed by processing the treated bauxite ore or treated Bayer product using one or more processes associated with the Bayer process results in an increased yield of alumina product, increased alumina content (purity) in the alumina product obtained, or both when compared to the same bauxite ore or Bayer product subjected to the same process(es) but in the absence of a boronic acid functional compound.
Claims9
A method of increasing the yield of alumina from a bauxite ore, the process comprising:
- combining the bauxite ore with water to form a bauxite slurry,
- adding an effective amount of boronic acid functional polymer to the bauxite slurry to form a treated slurry;
- and
- processing the treated slurry to yield an alumina product,
- wherein the method excludes adding compounds having 1,2-diol or 1,3-diol moieties to the bauxite slurry or the treated slurry;
- and
- wherein an effective amount of the boronic acid functional polymer is the amount of the boronic acid functional polymer added to the bauxite slurry to obtain a yield of alumina that is at least 0.5% higher by weight than the yield of alumina obtained from the corresponding untreated slurry processed according to the same process as the treated slurry.
A method comprising combining a composition with a bauxite ore, the composition comprising a boronic acid functional polymer and water and excluding polysaccharides.