Synthesis of porous graphitic carbon membranes
AssigneesQatar Foundation for Education, Science and Community Development, Total E&P Golfe Ltd
InventorsLei Fang, Sai Che, Chenxu Wang, Mohammed Al-Hashimi, Sarbajit Banerjee
Life of this patent
Estimating the term…
Abstract
Methods for preparation of a carbon membrane include providing a solution comprising a diacetyl biphenyl monomer and an alkylsulfonic acid. The solution is treated under such conditions that an aldol condensation reaction occurs so as to produce a porous polymer network. The porous polymer network is treated under such conditions that a Scholl reaction occurs.
Claims17
A method for preparation of a carbon membrane, the method comprising:
- providing a first solution comprising a diacetyl biphenyl monomer and an alkylsulfonic acid;
- treating the first solution under such conditions that an aldol condensation reaction occurs to produce a porous polymer network;
- treating the porous polymer network under such conditions that a Scholl reaction occurs;
- synthesizing a porous carbon precursor;
- and
- wherein the synthesizing of the porous carbon precursor comprises:
- heating the first solution to a temperature between 100° C. and 200° C.;
- cooling the first solution;
- and
- extracting the porous carbon precursor;
- synthesizing a porous graphitic carbon;
- the synthesizing of the porous graphitic carbon comprises:
- providing a suspension comprising the porous carbon precursor;
- bubbling the suspension with N2;
- adding to the suspension a mixture comprising FeCl3 and MeNO2 dropwise;
- and
- stirring the suspension.
A method for preparation of a carbon membrane, the method comprising:
- providing a first solution comprising a diacetyl biphenyl monomer and an alkylsulfonic acid;
- treating the first solution under such conditions that an aldol condensation reaction occurs to produce a porous polymer network;
- treating the porous polymer network under such conditions that a Scholl reaction occurs;
- synthesizing a porous carbon precursor;
- and
- wherein the synthesizing of the porous carbon precursor comprises:
- heating the first solution to a temperature between 100° C. and 200° C.;
- cooling the first solution;
- and
- extracting the porous carbon precursor;
- synthesizing a porous graphitic carbon;
- the synthesizing of the porous graphitic carbon comprises:
- providing a suspension comprising the porous carbon precursor;
- bubbling the suspension with N2;
- adding to the suspension a mixture comprising FeCl3 and MeNO2 dropwise;
- and
- stirring the suspension;
- and
- wherein the diacetyl biphenyl monomer allows for the preparation of conductive, graphitic carbon materials.