# US 12,119,498 B2 · One-sided electrode with reduced twisting for a secondary battery, and method for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 12,119,498 B2
- Document ID: US12119498B2
- Status: Granted
- Kind: B2
- Application number: 16/491,083
- Filed: 2018-10-24
- Published: 2020-01-09
- Granted: 2024-10-15
- Earliest claimed: 2017-10-25
- Assignees: LG Energy Solution, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Sei Woon Oh; Yeo Kyung Yoon; Sun Hwak K. Woo; Yu Ra Jeong
- Web page: https://patentgrep.com/patent/US12119498B2

## CPC

- H01M 4/667: {in the form of layers, e.g. coatings}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/0435: {Rolling or calendering}
- H01M 4/13: Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
- H01M 4/139: Processes of manufacture
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 4/668: {Composites of electroconductive material and synthetic resins}
- H01M 4/669: {Steels}
- H01M 4/70: characterised by shape or form
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/052: Li-accumulators
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention provides a one-sided electrode for a secondary battery comprising a current collector, an electrode mixture layer applied to one surface of the current collector, and an electrode distortion-preventing layer formed on the other surface of the current collector to which no electrode mixture is applied. The one-sided electrode according to the present invention exhibits significantly reduced warping or curling after a rolling process and has the advantages of facilitating subsequent processes and enabling enhanced productivity.

## Claims

### Claim 1

A lithium secondary battery comprising a one-sided electrode, comprising:
a current collector;
an electrode mixture layer applied on one surface of the current collector, wherein a surface of the electrode mixture layer opposing the one surface of the current collector is exposed;
an electrode distortion-preventing layer disposed on an entire surface of an other side of the current collector on which no electrode mixture is applied such that the current collector is not exposed; and
an insulating polymer layer disposed on the electrode distortion-preventing layer on a surface of an other side of the electrode distortion-preventing layer on which no current collector is disposed,
wherein the electrode includes only one current collector,
the electrode mixture layer comprises an electrode active material, a conductive material, and a binder,
the electrode distortion-preventing layer is made of a metal that is different from a material of the current collector,
the insulating polymer layer is disposed on an entire surface of the electrode distortion-preventing layer,
the current collector includes copper, the electrode distortion-preventing layer does not include nickel,
the electrode distortion-preventing layer includes stainless steel or titanium, and
a thickness of the electrode distortion-preventing layer is thicker than a thickness of the current collector.

### Claim 2 (depends on 1)

The lithium secondary battery of claim 1, wherein a thickness of the electrode mixture layer is between 40 μm and 300 μm.

### Claim 3 (depends on 1)

The lithium secondary battery of claim 1, wherein the current collector and the electrode distortion-preventing layer are integrally formed as a clad metal.

### Claim 4 (depends on 3)

The lithium secondary battery of claim 3, wherein the clad metal includes two or more selected from the group consisting of copper, titanium, nickel, stainless steel, and an alloy thereof.

### Claim 5 (depends on 3)

The lithium secondary battery of claim 3, wherein the clad metal includes copper and stainless steel.

### Claim 6 (depends on 1)

The lithium secondary battery of claim 1, wherein a tensile strength of the electrode distortion-preventing layer is 80% to 120% of a tensile strength of the electrode mixture layer.

### Claim 7 (depends on 1)

The lithium secondary battery of claim 1, wherein the insulating polymer is made of one or more selected from the group consisting of polyethylene, polypropylene, polybutylene, polystyrene, polyethylene terephthalate, natural rubber, and synthetic rubber.

### Claim 8 (depends on 1)

The lithium secondary battery of claim 1, wherein the electrode is a negative electrode.

### Claim 9 (depends on 1)

The lithium secondary battery of claim 1, wherein the one-sided electrode includes only one insulating polymer layer.

### Claim 10 (depends on 1)

The lithium secondary battery of claim 1, wherein the electrode mixture layer does not include a silicon alloy.

### Claim 11 (depends on 1)

The lithium secondary battery of claim 1, wherein the insulating polymer layer comprises polybutylene (PB), polystyrene (PS), natural rubber or synthetic rubber.

### Claim 12 (depends on 1)

The lithium secondary battery of claim 1, wherein the insulating polymer layer is directly disposed on the entire surface of the electrode distortion-preventing layer.

### Claim 13 (depends on 1)

The lithium secondary battery of claim 1, wherein the electrode distortion-preventing layer includes stainless steel.

### Claim 14 (depends on 1)

The lithium secondary battery of claim 1, wherein the electrode distortion-preventing layer includes titanium.

### Claim 15 (depends on 1)

A method of manufacturing the lithium secondary battery according to claim 1, comprising the steps of:
(a) laminating the electrode distortion-preventing layer on the one surface of the current collector and subsequently applying heat and pressure;
(b) applying an electrode active material slurry including an electrode active material and a solvent on the other surface of the current collector;
(c) drying the electrode coated with the electrode active material slurry; and
(d) rolling the electrode to have a predetermined thickness.

### Claim 16 (depends on 15)

The method of claim 15, further comprising a step of applying a polymer solution or attaching a polymer sheet on the electrode distortion-preventing layer between the steps (a) and (b).