Composite material pallet assembly formed from recycled material
OwnerPrakash Gowdarinventor
Life of this patent
Estimating the term…
Abstract
A pallet is formed in which one or more components thereof is formed of a composite material. The composite material includes mass particles consisting of a fibrous material derived at least in part from recycled post-consumer materials and a binding material consisting of a thermoplastic material derived at least in part from recycled post-consumer materials. The mass particles and the binding material are mixed such that the binding material is liquified and each mass particle is fully encapsulated by the liquified binding material.
Claims18
A method of forming a composite component in a pallet assembly comprising a pallet frame having a width spanning in a lateral direction between opposing sides of the pallet assembly, a length spanning in a longitudinal direction perpendicularly to the lateral direction between opposing ends of the pallet assembly, an upper deck frame defining a top of the pallet frame, a lower deck frame defining a bottom of the pallet frame, and a spacer frame including spacer members supporting the upper deck frame spaced above the lower deck frame, in which the upper deck frame includes two upper lead boards extending across the width of the pallet frame at the ends of the pallet frame and a plurality of cross members extending across the width of the pallet frame in between the upper lead boards, and in which at least one of the lead boards or the spacer members consists of the composite component, the method comprising:
- deriving a plurality of mass particles consisting of a fibrous material at least in part from recycled post-consumer materials such that the mass particles have an average particle size in the range of 1 to 50 millimeters;
- deriving a binding material consisting of a thermoplastic material at least in part from recycled post-consumer materials;
- mixing the mass particles and the binding material such that the mass particles occupy between 35% and 60% by weight of the composite component and the binding material occupies between 40% and 60% by weight of the composite component;
- heating the binding material before or during mixing such that the binding material is substantially liquified and each mass particle is substantially fully encapsulated by the liquified binding material;
- pressing the encapsulated mass particles together to form a block of material;
- and
- shaping the block of material to form the composite component by cutting the block of material to produce cuttings, and mixing the cuttings with the mass particles and the binding material in the formation of a second composite component.
A method of forming a composite component in a pallet assembly comprising a pallet frame having a width spanning in a lateral direction between opposing sides of the pallet assembly, a length spanning in a longitudinal direction perpendicularly to the lateral direction between opposing ends of the pallet assembly, an upper deck frame defining a top of the pallet frame, a lower deck frame defining a bottom of the pallet frame, and a spacer frame including spacer members supporting the upper deck frame spaced above the lower deck frame, in which the upper deck frame includes two upper lead boards extending across the width of the pallet frame at the ends of the pallet frame and a plurality of cross members extending across the width of the pallet frame in between the upper lead boards, and in which at least one of the lead boards or the spacer members consists of the composite component, the method comprising:
- deriving a plurality of mass particles consisting of a fibrous material at least in part from recycled post-consumer materials such that the mass particles have an average particle size in the range of 1 to 50 millimeters;
- deriving a binding material consisting of a thermoplastic material at least in part from recycled post-consumer materials;
- mixing the mass particles and the binding material such that the mass particles occupy between 35% and 60% by weight of the composite component and the binding material occupies between 40% and 60% by weight of the composite component;
- heating the binding material before or during mixing such that the binding material is substantially liquified and each mass particle is substantially fully encapsulated by the liquified binding material;
- cooling the encapsulated mass particles;
- transporting the encapsulated mass particles to a secondary manufacturing location;
- heating the encapsulated mass particles at the secondary manufacturing location;
- and pressing the encapsulated mass particles to form a block of material and shaping the block of material to form the composite component at the secondary manufacturing location.
A method of forming a composite component in a pallet assembly comprising a pallet frame having a width spanning in a lateral direction between opposing sides of the pallet assembly, a length spanning in a longitudinal direction perpendicularly to the lateral direction between opposing ends of the pallet assembly, an upper deck frame defining a top of the pallet frame, a lower deck frame defining a bottom of the pallet frame, and a spacer frame including spacer members supporting the upper deck frame spaced above the lower deck frame, in which the upper deck frame includes two upper lead boards extending across the width of the pallet frame at the ends of the pallet frame and a plurality of cross members extending across the width of the pallet frame in between the upper lead boards, and in which at least one of the lead boards or the spacer members consists of the composite component, the method comprising:
- deriving a plurality of mass particles consisting of a fibrous material at least in part from recycled post-consumer materials such that the mass particles have an average particle size in the range of 1 to 50 millimeters;
- deriving a binding material consisting of a thermoplastic material at least in part from recycled post-consumer materials;
- mixing the mass particles and the binding material such that the mass particles occupy between 35% and 60% by weight of the composite component and the binding material occupies between 40% and 60% by weight of the composite component;
- heating the binding material during the mixing such that the binding material undergoes partial pyrolysis and such that the binding material is substantially liquified and each mass particle is substantially fully encapsulated by the liquified binding material;
- pressing the encapsulated mass particles together to form a block of material;
- and
- shaping the block of material to form the composite component.
A method of forming a composite component in a pallet assembly comprising a pallet frame having a width spanning in a lateral direction between opposing sides of the pallet assembly, a length spanning in a longitudinal direction perpendicularly to the lateral direction between opposing ends of the pallet assembly, an upper deck frame defining a top of the pallet frame, a lower deck frame defining a bottom of the pallet frame, and a spacer frame including spacer members supporting the upper deck frame spaced above the lower deck frame, in which the upper deck frame includes two upper lead boards extending across the width of the pallet frame at the ends of the pallet frame and a plurality of cross members extending across the width of the pallet frame in between the upper lead boards, and in which at least one of the lead boards or the spacer members consists of the composite component, the method comprising:
- deriving a plurality of mass particles consisting of a fibrous material at least in part from recycled post-consumer materials such that the mass particles have an average particle size in the range of 1 to 50 millimeters;
- deriving a binding material consisting of a thermoplastic material at least in part from recycled post-consumer materials;
- mixing the mass particles and the binding material such that the mass particles occupy between 35% and 60% by weight of the composite component and the binding material occupies between 40% and 60% by weight of the composite component;
- heating the binding material before or during mixing such that the binding material is substantially liquified and each mass particle is substantially fully encapsulated by the liquified binding material;
- pressing the encapsulated mass particles together to form a block of material;
- and
- shaping the block of material to form the composite component;
- wherein the composite component is substantially non-porous.
A method of forming a composite component in a pallet assembly comprising a pallet frame having a width spanning in a lateral direction between opposing sides of the pallet assembly, a length spanning in a longitudinal direction perpendicularly to the lateral direction between opposing ends of the pallet assembly, an upper deck frame defining a top of the pallet frame, a lower deck frame defining a bottom of the pallet frame, and a spacer frame including spacer members supporting the upper deck frame spaced above the lower deck frame, in which the upper deck frame includes two upper lead boards extending across the width of the pallet frame at the ends of the pallet frame and a plurality of cross members extending across the width of the pallet frame in between the upper lead boards, and in which at least one of the lead boards or the spacer members consists of the composite component, the method comprising:
- deriving a plurality of mass particles consisting of a fibrous material at least in part from recycled post-consumer materials such that the mass particles have an average particle size in the range of 1 to 50 millimeters;
- deriving a binding material consisting of a thermoplastic material at least in part from recycled post-consumer materials;
- mixing the mass particles and the binding material such that the mass particles occupy between 35% and 60% by weight of the composite component and the binding material occupies between 40% and 60% by weight of the composite component;
- heating the binding material before or during mixing such that the binding material is substantially liquified and each mass particle is substantially fully encapsulated by the liquified binding material;
- pressing the encapsulated mass particles together to form a block of material;
- and
- shaping the block of material to form the composite component;
- wherein any voids in the composite component are smaller in size that the average particle size of the mass particles.
A method of forming a composite component in a pallet assembly comprising a pallet frame having a width spanning in a lateral direction between opposing sides of the pallet assembly, a length spanning in a longitudinal direction perpendicularly to the lateral direction between opposing ends of the pallet assembly, an upper deck frame defining a top of the pallet frame, a lower deck frame defining a bottom of the pallet frame, and a spacer frame including spacer members supporting the upper deck frame spaced above the lower deck frame, in which the upper deck frame includes two upper lead boards extending across the width of the pallet frame at the ends of the pallet frame and a plurality of cross members extending across the width of the pallet frame in between the upper lead boards, and in which at least one of the lead boards or the spacer members consists of the composite component, the method comprising:
- deriving a plurality of mass particles consisting of a fibrous material at least in part from recycled post-consumer materials such that the mass particles have an average particle size in the range of 1 to 50 millimeters;
- deriving a binding material consisting of a thermoplastic material at least in part from recycled post-consumer materials;
- mixing the mass particles and the binding material such that the mass particles occupy between 35% and 60% by weight of the composite component and the binding material occupies between 40% and 60% by weight of the composite component;
- heating the binding material before or during mixing such that the binding material is substantially liquified and each mass particle is substantially fully encapsulated by the liquified binding material;
- pressing the encapsulated mass particles together to form a block of material;
- and
- shaping the block of material to form the composite component;
- wherein an average thickness of the encapsulating binding material about the mass particles is less than the average particle size of the mass particles.
A method of forming a composite component in a pallet assembly comprising a pallet frame having a width spanning in a lateral direction between opposing sides of the pallet assembly, a length spanning in a longitudinal direction perpendicularly to the lateral direction between opposing ends of the pallet assembly, an upper deck frame defining a top of the pallet frame, a lower deck frame defining a bottom of the pallet frame, and a spacer frame including spacer members supporting the upper deck frame spaced above the lower deck frame, in which the upper deck frame includes two upper lead boards extending across the width of the pallet frame at the ends of the pallet frame and a plurality of cross members extending across the width of the pallet frame in between the upper lead boards, and in which at least one of the lead boards or the spacer members consists of the composite component, the method comprising:
- deriving a plurality of mass particles consisting of a fibrous material at least in part from recycled post-consumer materials such that the mass particles have an average particle size in the range of 1 to 50 millimeters;
- deriving a binding material consisting of a thermoplastic material at least in part from recycled post-consumer materials;
- mixing the mass particles and the binding material such that the mass particles occupy between 35% and 60% by weight of the composite component and the binding material occupies between 40% and 60% by weight of the composite component;
- heating the binding material before or during mixing such that the binding material is substantially liquified and each mass particle is substantially fully encapsulated by the liquified binding material;
- pressing the encapsulated mass particles together to form a block of material;
- and
- shaping the block of material to form the composite component;
- wherein the mass particles consist only of particles formed of cellulose fibres.
A method of forming a composite component in a pallet assembly comprising a pallet frame having a width spanning in a lateral direction between opposing sides of the pallet assembly, a length spanning in a longitudinal direction perpendicularly to the lateral direction between opposing ends of the pallet assembly, an upper deck frame defining a top of the pallet frame, a lower deck frame defining a bottom of the pallet frame, and a spacer frame including spacer members supporting the upper deck frame spaced above the lower deck frame, in which the upper deck frame includes two upper lead boards extending across the width of the pallet frame at the ends of the pallet frame and a plurality of cross members extending across the width of the pallet frame in between the upper lead boards, and in which at least one of the lead boards or the spacer members consists of the composite component, the method comprising:
- deriving a plurality of mass particles consisting of a fibrous material at least in part from recycled post-consumer materials such that the mass particles have an average particle size in the range of 1 to 50 millimeters;
- deriving a binding material consisting of a thermoplastic material at least in part from recycled post-consumer materials;
- mixing the mass particles and the binding material such that the mass particles occupy between 35% and 60% by weight of the composite component and the binding material occupies between 40% and 60% by weight of the composite component;
- heating the binding material before or during mixing such that the binding material is substantially liquified and each mass particle is substantially fully encapsulated by the liquified binding material;
- pressing the encapsulated mass particles together to form a block of material;
- and
- shaping the block of material to form the composite component;
- wherein the composite material is substantially non-porous;
- wherein any voids in the composite material are smaller in size that the average particle size of the mass particles;
- wherein an average thickness of the encapsulating binding material about the mass particles is less than the average particle size of the mass particles;
- wherein the binding material has a pyrolysis temperature which is lower than a pyrolysis temperature of the mass particles;
- and
- wherein the composite material has a density in a range of 0.75 to 0.95 grams per cubic centimeter.
Dependencies are inferred from the claim text.