Recycled oil and rubber modified for asphalt and method of use
AssigneeKenneth Grzybowski
InventorKenneth F. Grzybowski
Life of this patent
Estimating the term…
Abstract
A asphalt binder modifier or a stand-alone asphalt binder and the method of making the asphalt binder or binder modifier are disclosed. The asphalt modifier or binder consisting of treated re-refined engine oil bottoms/VTB's treated by injecting air into re-refining engine oil bottoms/VTB's at temperatures between 150° F. and 550° F. The re-refined engine oil can be processed with ground tire rubber. The binder modifier was blended with various paving and roofing asphalts to form performance-enhanced modified asphalt binders used in paving, roofing, and industrial products.
Claims18
A modifier for asphalt comprising re-refined engine oil, ground tire rubber and at least one plastomer and/or at least one elastomer, wherein the re-refined engine oil and ground tire rubber are oxidized by heating the re-refined engine oil and ground tire rubber to a temperature of about 150° F. to about 550° F. or to 50° F. below the flash point of the re-refined engine oil and injecting air into the re-refined engine oil and ground tire rubber while mixing, wherein after oxidation the modifier has a softening point of at least 150° F. and penetration values that vary by 75 decimillimeters or less when measured at about 39° F. and about 115° F.
An asphalt modifier emulsion comprising re-refined engine oil, ground tire rubber, and water, wherein the re-refined engine oil and ground tire rubber are oxidized by heating the re-refined engine oil and ground tire rubber to a temperature of about 150° F. to about 550° F. or to 50° F. below the flash point of the re-refined engine oil and injecting air into the re-refined engine oil and ground tire rubber while mixing, wherein after oxidation the modifier has a softening point of at least 150° F. and penetration values that vary by 75 decimillimeters or less when measured at about 39° F. and about 115° F.
A modifier for asphalt comprising re-refined engine oil, ground tire rubber and at least one wax, wherein the re-refined engine oil and ground tire rubber are oxidized by heating the re-refined engine oil and ground tire rubber to a temperature of about 150° F. to about 550° F. or to 50° F. below the flash point of the re-refined engine oil and injecting air into the re-refined engine oil and ground tire rubber while mixing, wherein after oxidation the modifier has a softening point of at least 150° F. and penetration values that vary by 75 decimillimeters or less when measured at about 39° F. and about 115° F.
A modifier for asphalt comprising re-refined engine oil, ground tire rubber and at least one polymer, wherein the re-refined engine oil and ground tire rubber are oxidized by heating the re-refined engine oil and ground tire rubber to a temperature of about 150° F. to about 550° F. or to 50° F. below the flash point of the re-refined engine oil and injecting air into the re-refined engine oil and ground tire rubber while mixing, wherein after oxidation the modifier has a softening point of at least 150° F. and penetration values that vary by 75 decimillimeters or less when measured at about 39° F. and about 115° F.