Cementitious mixture and method of making the same
AssigneeKing Saud University
InventorsGalal Fares, Mohammad Iqbal Khan
Life of this patent
Estimating the term…
Loading patent…
AssigneeKing Saud University
InventorsGalal Fares, Mohammad Iqbal Khan
Estimating the term…
The cementitious mixture includes cement with a concentration of between about 5 wt % and about 20 wt %; powdered glass with a concentration of between about 5 wt % and about 35 wt %; fly ash with a concentration of between about 20 wt % and about 40 wt %; sand with a concentration of between about 18 wt % and about 25 wt %; a poly(carboxylate ether)-based superplasticizer with a concentration of between about 0.8 wt % and about 1.2 wt %; and water with a concentration of between about 14 wt % and about 16 wt %. Alternatively, the fly ash may be replaced with ground granulated blast furnace slag (GGBFS). The powdered glass is preferably powdered recycled glass cullet. The glass cullet may be ground to have an average particle size of about 10 μm or less. The sand may be red dune sand, and the cement may be Portland cement or white cement. The cementitious may also include polyvinyl alcohol (PVA) microfibers.
A cementitious mixture, comprising:
A cementitious mixture, comprising:
A method of making a cementitious mixture, comprising the steps of:
Dependencies are inferred from the claim text.