US 11,905,206 B2Granted
Binders and materials made therewith
AssigneesKnauf Insulation, Inc., Knauf Insulation SPRL
InventorsBrian Lee Swift, Ronald E. Kissell, Ruijian Xu
Life of this patent
Estimating the term…
Abstract
Binders to produce or promote cohesion in non-assembled or loosely assembled matter.
Claims17
A thermal or acoustical fiberglass insulation material comprising:
- (a) a collection of mineral fibers;
- and
- (b) a binder disposed on the collection of mineral fibers, wherein the binder comprises i) at least one reaction product of a reducing sugar reactant and an amine reactant, wherein the percent by dry weight of the reducing sugar reactant with respect to the total weight of reactants ranges from about 73% to about 96%, ii) a silicon-containing coupling agent, and iii) optionally, a corrosion inhibitor, wherein the fiberglass material comprises less than about 99% by weight and more than about 75% by weight mineral fibers, and wherein the fiberglass material has a density of from about 0.4 lbs/ft3 to about 6 lbs/ft3.
A thermal or acoustical fiberglass insulation material comprising:
- (a) a collection of mineral fibers;
- and
- (b) a binder disposed on the collection of mineral fibers, the binder comprising i) a mixture of Maillard reactants, wherein the percent by dry weight of a reducing sugar reactant with respect to the total weight of reactants ranges from about 73% to about 96%, ii) a silicon-containing coupling agent, and iii) optionally, a corrosion inhibitor, wherein the fiberglass material comprises less than about 99% by weight and more than about 75% by weight mineral fibers, and wherein the fiberglass material has a density in the range from about 0.4 lbs/ft3 to about 6 lbs/ft3.
A thermal or acoustical fiberglass insulation material comprising:
- (a) a collection of mineral fibers;
- and
- (b) a binder disposed on the collection of mineral fibers, wherein the binder comprises i) at least one reaction product of a reducing sugar reactant and a polycarboxylic acid ammonium salt reactant, wherein the percent by dry weight of the reducing sugar reactant with respect to the total weight of reactants ranges from about 73% to about 96%, ii) a silicon-containing coupling agent, and iii) optionally, a corrosion inhibitor, wherein the fiberglass material comprises less than about 99% by weight and more than about 75% by weight mineral fibers, and wherein the fiberglass material has a density in the range from about 0.4 lbs/ft3 to about 6 lbs/ft3.
Dependencies are inferred from the claim text.