# US 11,897,081 B2 · Method for polishing silicon substrate and polishing composition set

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,897,081 B2
- Document ID: US11897081B2
- Status: Granted
- Kind: B2
- Application number: 16/080,960
- Filed: 2017-02-13
- Published: 2019-02-28
- Granted: 2024-02-13
- Earliest claimed: 2016-03-01
- Assignees: Fujimi Incorporated
- Applicants: Fujimi Incorporated
- Inventors: Shinichiro Takami; Yusuke Kawasaki
- Web page: https://patentgrep.com/patent/US11897081B2

## CPC

- B24B 37/044: {characterised by the composition of the lapping agent}
- B24B 37/00: Lapping machines or devices; Accessories (B24B3/00 takes precedence)
- C09G 1/02: containing abrasives or grinding agents {(abrasives as such C09K3/14; polishing of semi-conductors H10P52/40)}
- C09K 3/1409: {Abrasive particles per se (preparation of diamond C01B32/25)}
- H10P 52/402: {of semiconductor materials}
- H10P 90/123: {by grinding or lapping}
- H10P 90/129: {by polishing}
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- C09G: POLISHING COMPOSITIONS (French polish C09F11/00); SKI WAXES
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Provided are a polishing method that can be commonly applied to different types of silicon substrates varying in resistivity as well as a polishing composition set used in the polishing method. The silicon substrate polishing method provided by this invention comprises supplying a first polishing slurry S1 and a second polishing slurry S2 to a silicon substrate to be polished, switching them in this order midway through polishing the silicon substrate. The first polishing slurry S1 comprises an abrasive A1 and a water-soluble polymer P1. The polishing removal rate of the first polishing slurry S1 is higher than that of the second polishing slurry S2.

## Claims

### Claim 1

A method for polishing silicon substrates consisting of a high-resistivity silicon substrate having a resistivity of 1 Ω·cm or greater and a low-resistivity silicon substrate having a resistivity less than 0.005 Ω·cm, the method comprising a stock polishing step and a final polishing step for each of the high-resistivity silicon substrate and the low-resistivity silicon substrate, wherein the final polishing step is a step polishing only a single side of each of the high-resistivity silicon substrate and the low-resistivity silicon substrate, the final polishing step comprising:
supplying a first polishing slurry S1 and a second polishing slurry S2 to the silicon substrate to be polished, switching them in this order midway through polishing a single side of the silicon substrate,
wherein the first polishing slurry S1 comprises an abrasive A1, a water-soluble polymer P1, and a basic compound B1, wherein:
the abrasive A1 has a BET diameter of 5 nm or greater and 100 nm or less and a true specific gravity of 1.5 or higher and 2.3 or lower, and a content of the abrasive A1 in the first polishing slurry S1 is 0.05% by weight or higher and 10% by weight or lower;
the water-soluble polymer P1 is a mixture of a water-soluble polymer having a vinyl alcohol-based polymer chain and a water-soluble polymer having an N-vinyl-based polymer chain, or the water-soluble polymer P1 is a copolymer having the vinyl alcohol-based polymer chain and the N-vinyl-based polymer chain in the same molecule, a content of the vinyl alcohol-based polymer chain in the water-soluble polymer P1 is 50% by weight or higher and an amount of the water-soluble polymer P1 per 1 g of abrasive A1 contained in the first polishing slurry S1 is 0.03 g or less;
the basic compound B1 is an alkali metal hydroxide comprising potassium hydroxide;
the first polishing slurry has a pH of 8.0 or higher and 12.0 or lower; and
the first polishing slurry S1 shows higher polishing removal rate than the second polishing slurry S2; and
wherein:
the first polishing slurry S1 for polishing the low-resistivity silicon substrate in the final polishing step has the same composition as the first polishing slurry S1 for polishing the high-resistivity silicon substrate in the final polishing step;
the second polishing slurry S2 for polishing the low-resistivity silicon substrate in the final polishing step has the same composition as the second polishing slurry S2 for polishing the high-resistivity silicon substrate in the final polishing step; and
the first polishing slurry S1 shows a first polishing removal rate for polishing the high-resistivity silicon substrate and a second polishing removal rate for polishing the low-resistivity silicon substrate, wherein the first polishing removal rate is less than or equal to 6.2 times the second polishing removal rate.

### Claim 2 (depends on 1)

The polishing method according to claim 1, wherein the first polishing slurry S1 comprises at least 0.001% water-soluble polymer P1 by weight.

### Claim 3 (depends on 1)

The polishing method according to claim 1, wherein the abrasive A1 has a BET diameter of 5 nm or greater and smaller than 60 nm.

### Claim 4 (depends on 1)

The polishing method according to claim 1, wherein the second polishing slurry S2 comprises an abrasive A2 and a water-soluble polymer P2, and the concentration of the water-soluble polymer P2 in the second polishing slurry S2 is higher than the concentration of the water-soluble polymer P1 in the first polishing slurry S1.

### Claim 5 (depends on 1)

The polishing method according to claim 1, wherein the second polishing slurry S2 comprises an abrasive A2, and the abrasive A2 content in the second polishing slurry S2 is 0.5% by weight or lower.

### Claim 6 (depends on 1)

A polishing composition used in the polishing method according to claim 1, wherein the polishing composition is the first polishing slurry S1 or a concentrate thereof.

### Claim 7 (depends on 1)

A polishing composition used in the polishing method according to claim 1, wherein the polishing composition is the second polishing slurry S2 or a concentrate thereof.

### Claim 8 (depends on 1)

A polishing composition set used in the polishing method according to claim 1, the polishing composition set comprising
the first polishing slurry S1 or a first composition Q1 which is a concentrate of S1, and
the second polishing slurry S2 or a second composition Q2 which is a concentrate of S2;
wherein
the first composition Q1 and the second composition Q2 are separately stored.

### Claim 9 (depends on 1)

The method of claim 1, wherein the water-soluble polymer P1 has a weight average molecular weight (Mw) of 20×104 or lower.

### Claim 10 (depends on 1)

The method of claim 1, wherein the water-soluble polymer P1 is the mixture of a water-soluble polymer having the vinyl alcohol-based polymer chain and the water-soluble polymer having the N-vinyl-based polymer chain.

### Claim 11 (depends on 10)

The method of claim 10, wherein the water-soluble polymer having the vinyl alcohol-based polymer chain has a weight average molecular weight (Mw) of 20×104 or lower, and the water-soluble polymer having the N-vinyl-based polymer chain has a Mw of 3×104 or higher but lower than the Mw of the water-soluble polymer having the vinyl alcohol-based polymer chain.

### Claim 12 (depends on 1)

The method of claim 1, wherein the water-soluble polymer P1 is the copolymer having the vinyl alcohol-based polymer chain and the N-vinyl-based polymer chain in one same molecule.

### Claim 13

A method for polishing silicon substrates consisting of a high-resistivity silicon substrate having a resistivity of 1 Ω·cm or greater and a low-resistivity silicon substrate having a resistivity less than 0.005 Ω·cm, the method comprising a stock polishing step and a final polishing step for each of the high-resistivity silicon substrate and the low-resistivity silicon substrate, wherein the final polishing step is a step polishing only a single side of each of the high-resistivity silicon substrate and the low-resistivity silicon substrate, the final polishing step comprising:
supplying a first polishing slurry S1 and a second polishing slurry S2 to the silicon substrate to be polished, switching them in this order midway through polishing a single side of the silicon substrate,
wherein the first polishing slurry S1 comprises an abrasive A1, a water-soluble polymer P1, and a basic compound B1, wherein:
the abrasive A1 has a BET diameter of 5 nm or greater and 100 nm or less and a true specific gravity of 1.5 or higher and 2.3 or lower, and a content of the abrasive A1 in the first polishing slurry S1 is 0.05% by weight or higher and 10% by weight or lower;
the water-soluble polymer P1 is a mixture of a water-soluble polymer having a vinyl alcohol-based polymer chain and a water-soluble polymer having an N-vinyl-based polymer chain, or the water-soluble polymer P1 is a copolymer having the vinyl alcohol-based polymer chain and the N-vinyl-based polymer chain in the same molecule, the N-vinyl-based polymer chain is a vinylpyrrolidone-based polymer and an amount of the water-soluble polymer P1 per 1 g of abrasive A1 contained in the first polishing slurry S1 is 0.03 g or less;
the basic compound B1 is an alkali metal hydroxide comprising potassium hydroxide;
the first polishing slurry S1 has a pH of 8.0 or higher and 12.0 or lower; and
the first polishing slurry S1 shows higher polishing removal rate than the second polishing slurry S2; and
wherein:
the first polishing slurry S1 for polishing the low-resistivity silicon substrate in the final polishing step has the same composition as the first polishing slurry S1 for polishing the high-resistivity silicon substrate in the final polishing step;
the second polishing slurry S2 for polishing the low-resistivity silicon substrate in the final polishing step has the same composition as the second polishing slurry S2 for polishing the high-resistivity silicon substrate in the final polishing step; and
the first polishing slurry S1 shows a first polishing removal rate for polishing the high-resistivity silicon substrate and a second polishing removal rate for polishing the low-resistivity silicon substrate, wherein the first polishing removal rate is less than or equal to 6.2 times the second polishing removal rate.