A coating film is provided in a cable, a medical hollow tube, a molded article and a hollow tube. The coating film is formed from a rubber composition including a rubber component and fine particles. A static friction coefficient on a surface of the coating film is 0.5 or less. When the coating film is subjected to a testing such that a long fiber non-woven fabric including cotton linters including an alcohol for disinfection with a length of 50 mm along a wiping direction is brought contiguous to the surface of the coating film at a shearing stress of 2×10−3 MPa to 4×10−3 MPa, followed by wiping off the surface of the coating film at a speed of 80 times/min to 120 times/min and 20,000 repetitions thereof for a wiping direction length of 150 mm, a difference (an absolute value of a difference) between the static friction coefficients of the coating film before and after the testing is not greater than 0.1.
A method for manufacturing a molded article comprising a molded article main body, and a coating film covering a surface of the molded article main body, the coating film adhering to the molded article main body, the method comprising:
Dependencies are inferred from the claim text.