Precipitated silica and process for its manufacture
AssigneeRhodia Operations
InventorsEmmanuelle Allain Najman, Fabien Stocklouser, Pascaline Garbey, Caroline Fayolle, Sylvaine Neveu, Laurent Guy
Life of this patent
Estimating the term…
Loading patent…
AssigneeRhodia Operations
InventorsEmmanuelle Allain Najman, Fabien Stocklouser, Pascaline Garbey, Caroline Fayolle, Sylvaine Neveu, Laurent Guy
Estimating the term…
A precipitated silica having a broad particle size distribution and large median particle size as well as its method of manufacture is provided. The precipitated silica has a CTAB surface area SCTAB in the range from 40 to 300 m2/g, a difference between BET surface area SBET and CTAB surface area SCTAB of at least 35 m2/g, a width of the particle size distribution Ld, measured by centrifugal sedimentation, of at least 1.5, an amount of aluminium WA1 in the range from 0.5 to 7.0 wt %, and a median particle size d50, measured by centrifugal sedimentation, such that for a given value of CTAB surface area SCTAB and amount of aluminium WAl, parameter A, defined by the following equation: A=|d50|+0.782×|SCTAB|−8.524×|WAl|.
A precipitated silica characterised by: