Process for manufacturing toroid parts
AssigneeKeystone Powdered Metal Company
InventorsGary L. Anderson, Peter G. Imbrogno, Kevin Brunner
Life of this patent
Estimating the term…
Abstract
It has been found that duplex monolithic parts can be manufactured in high volume at low cost by using powder metal technology to mold and sinter an inner component of the part into an outer component of the part. This technique reduces the cost of manufacturing intricate metal products by taking advantage of the attributes of powder metal technology in making the inner component of the part. The outer component of the part can be wrought machined, stamped or forged, or made by double press double sinter or forging a powder metal component of the part. In any case, this technique can beneficially be used in making a wide variety of toroid parts, such as gears, clutches, sprags, bearing races, one-way diodes, and the like.
Claims12
A metal ring with an outer higher strength component and an inner component wherein the inner component is sintered into the outer component of the ring, wherein the outer component is a wrought metal which is comprised of a cast metal having a density which is within the range of 7.8 g/cc to 7.85 g/cc, and wherein the inner component is comprised of a sintered powder metal and has a density which is within the range of 6.6 g/cc to 7.3 g/cc.
A metal ring with an outer higher strength component and an inner component wherein the inner component is sintered into the outer component of the ring, wherein the outer component is comprised of a wrought metal having a density which is within the range of 7.8 g/cc to 7.85 g/cc, wherein the inner component has a density which is within the range of 6.6 g/cc to 7.3 g/cc, wherein the inner component is a one-way clutch and wherein the outer component is a helical gear.
Dependencies are inferred from the claim text.