Environment-friendly hot-melt composition for vehicle interior material
AssigneesHyundai Motor Company, Kia Corporation, MUJIN, Inc.
InventorsJin Uk Hwang, Seung Keon Woo, Jae Hong Woo
Life of this patent
Estimating the term…
Abstract
Disclosed is an environment-friendly hot-melt composition for a vehicle interior material, the hot-melt composition including: 65 wt % to 85 wt % of an aromatic polyamide; 10 wt % to 30 wt % of an aliphatic polyamide; 1 wt % to 5 wt % of an olefinic elastomer graft-polymerized with maleic anhydride; and 0.1 wt % to 2 wt % of an antioxidant.
Claims10
A hot-melt composition comprising:
- 65 wt % to 85 wt % of an aromatic polyamide;
- 10 wt % to 30 wt % of an aliphatic poly amide;
- and
- 1 wt % to 5 wt % of an olefinic elastomer graft-polymerized with maleic anhydride,
- wherein the hot-melt composition has a first melting-point peak observed at 40° C. to 60° C. and a second melting-point peak observed at 100° C. to 110° C. upon thermal analysis using differential scanning calorimetry (DSC).
2 more elements
A vehicle interior material comprising:
- a substrate;
- an adhesive layer comprising a hot-melt composition and disposed on the substrate, the hot-melt composition comprising:
- 65 wt % to 85 wt % of an aromatic polyamide,
- 10 wt % to 30 wt % of an aliphatic polyamide, and
- 1 wt % to 5 wt % of an olefinic elastomer graft-polymerized with maleic anhydride;
- and
- a skin layer disposed on the adhesive layer,
- wherein the hot-melt composition has a first melting-point peak observed at 40° C. to 60° C. and a second melting-point peak observed at 100° C. to 110° C. upon thermal analysis using differential scanning calorimetry (DSC).