Air-filter media comprising a relofted spunbonded web, and methods of making and using
Assignee3M Innovative Properties Company
InventorsZhiqun Zhang, Edward Keith Willis, Jacob J. Thelen, Daniel E. Johnson, Bryan L. Gerhardt, Michael R. Berrigan
Life of this patent
Estimating the term…
Abstract
A relofted, spunbonded nonwoven web exhibiting a solidity of from less than 8.0%, to at least 3.0%, and exhibiting a Quality Factor of at least 0.30. Methods of making a relofted web; and, methods of using a relofted web as an air-filtration web, e.g. as a filter media or a layer thereof.
Claims23
An air-filter media comprising a relofted, spunbonded nonwoven web exhibiting a solidity of from less than 8.0%, to at least 3.0%, and exhibiting a Quality Factor of at least 0.30.
A process of relofting a spunbonded precursor web, the process comprising:
- mechanically working a spunbonded precursor web that comprises a solidity of no more than 10%, to produce a relofted, spunbonded air-filtration web comprising a solidity of from less than 8.0%, to at least 3.0%, and comprising a Quality Factor of at least 0.30.