Method of manufacturing a composite material that is used to make blocks, bricks, tiles, or pavers
OwnerJose Miguel Martinez Torres, Daniel Andres Gonzalez Guevara +1inventors
InventorsJose Miguel Martinez Torres, Daniel Andres Gonzalez Guevara, Edison David Coloma Maldonado
Life of this patent
Estimating the term…
Abstract
A method of manufacturing a composite material that is used to make blocks, bricks, tiles, or payers. The method comprises of making a liquid conglomerate material, of making a solid conglomerate material, of mixing the liquid conglomerate material and the solid conglomerate material together to make the composite material, and lastly of pressing the composite material into either a block, a brick, a tile, or a paver.
Claims2
A method of manufacturing a composite material that is used to make blocks, bricks, tiles, or pavers, the method comprises the steps of:
- providing a plastic resin that is water impermeable and that is free of chloride;
- providing a vinyl acrylic emulsion that has fifty percent of solids;
- providing a mixer;
- mixing the plastic resin and the acrylic vinyl emulsion for at least five minutes in the mixer, thereby creating a liquid conglomerate material, the liquid conglomerate material consists of, by volume, sixty percent of the acrylic vinyl emulsion and forty percent of the vinyl acrylic emulsion;
- providing a blended cement material that consists of, by weight, between 15 percent to thirty-five percent of a pozzolanic material, four percent of a gypsum material, and a clinker material, the blended cement will have a total weight of one hundred percent;
- providing a hydrated lime material;
- providing a natural dye material;
- providing a mixer;
- mixing the blended cement material, the hydrated lime material, and the natural dye material for at least five minutes in the mixer, thereby creating a solid conglomerate material, the solid conglomerate material consists of eighty percent of the blended cement material, fifteen percent of the hydrated lime material, and five percent of the natural dye material;
- providing a soil material;
- providing a water material;
- finding a site of where to install a manufacturing plant that will manufacture the composite material, the site is chosen based on the soil material that covers the site;
- analyzing the soil of the site to determine if the soil is adequate to make the composite material;
- choosing the site if the soil on the site is thirty percent of a clay soil, forty-five percent of a silt-type soil, and twenty-five percent of a coarse sand that is between three mm to 4 mm thick;
- preparing the soil so that is has a humidity that is from at least six percent to at most seven percent humidity;
- providing a mixer mill;
- mixing the soil and the solid conglomerate for at least five minutes in the mixer mill, thereby creating a soil and solid conglomerate mix, the soil and solid conglomerate mix consists of eighty-five percent of the soil and fifteen percent of the solid conglomerate material by weight;
- mixing the liquid conglomerate material with the soil and solid conglomerate mix for at least five minutes in the mixer mill at a humidity that is at least nine percent to ten percent moisture thereby creating the composite material, the composite material consists of eighty-five percent of the soil and solid conglomerate mix and fifteen percent of the liquid conglomerate material;
- providing an industrial press;
- and
- pressing the composite material in the industrial press at a pressure that is at least 2800 pounds per square inch to either form either a block, a brick, a tile, or a paver.
Dependencies are inferred from the claim text.