Black heart malleable cast-iron and method for manufacturing same
AssigneeProterial, Ltd.
InventorsRyo Goto, Takayuki Fukaya, Hiroshi Matsui, Kenta Matsuura
Life of this patent
Estimating the term…
Loading patent…
AssigneeProterial, Ltd.
InventorsRyo Goto, Takayuki Fukaya, Hiroshi Matsui, Kenta Matsuura
Estimating the term…
Provided is a black heart malleable cast iron and a method for manufacturing the same which can significantly shorten the time required for graphitization, as compared with the prior art. The black heart malleable cast iron includes a matrix of ferrite and lump graphite included in the matrix, and includes at least one selected from the group consisting of (i) 0.0050% by mass or more and 0.15% by mass or less of bismuth and 0.020% by mass or more of manganese, and (ii) 0.0050% by mass or more and 1.0% by mass or less of aluminum and 0.0050% by mass or more of nitrogen. In addition, the grain size of the matrix is 8.0 or more and 10.0 or less in terms of grain size number, numerically determined by comparison between a metallographic photograph of the matrix and a standard grain size chart.
A black heart malleable cast iron comprising a matrix of ferrite and lump graphite included in the matrix, the black heart malleable cast iron comprising:
Dependencies are inferred from the claim text.