A leather tanning method using chrome-free and formaldehyde-free adhesive pertains to the technical field of leather tanning, in which the quaternary ammonium salt cationic resin adhesive is used for leather pretanning and retanning. After drying, the leather has excellent performance, which is comparable to traditional chrome and formaldehyde tanned leather. The method solves the drawbacks of using chromium and formaldehyde tanning agents in the leather tanning industry, which pollutes the environment and raises health concerns. The present disclosure has obvious advantages in environmental protection, huge industrial application value, and has broad application prospects.
Claims7
A leather tanning method using chrome-free and formaldehyde-free adhesive comprising:
- 1) mixing quaternary ammonium polymer with water to prepare a quaternary ammonium polymer solution with a mass concentration of 5-35%;
- 2) putting animal hide or skin in an acid solution containing sodium chloride and soaking the animal hide or skin for 24 hours, then drying the animal hide or skin at a room temperature;
- 3) placing dried animal hide or skin in a rotary drum, adding the quaternary ammonium polymer solution, and running the rotary drum at 10 rpm at room temperature in a forward direction for 15 minutes, in a reverse direction for 15 minutes, then in the forward direction again for 15 minutes, and in the reverse direction again for 15 minutes;
- 4) raising the temperature of the rotary drum to 40° C., running the rotary drum at 8 rpm in the forward direction for 15 minutes, in the reverse direction for 15 minutes, then in the forward direction again for 15 minutes, and in the reverse direction again for 15 minutes;
- 5) stopping rotation of the rotary drum and soaking the animal hide or skin for 12 hours;
- 6) adding an alkaline solution to adjust a system pH to 6.5-8, running the rotary drum at 8 rpm at room temperature in the forward direction for 5 minutes, in the reverse direction for 5 minutes, then in the forward direction again for 5 minutes, and in the reverse direction again for 5 minutes;
- 7) taking the resulting animal hide or skin out to dry at room temperature and obtain a leather product.
Dependencies are inferred from the claim text.