# US 11,697,612 B2 · Low LOI tellurium-lithium-silicon-zirconium frit system and conductive paste and application thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,697,612 B2
- Document ID: US11697612B2
- Status: Granted
- Kind: B2
- Application number: 17/680,878
- Filed: 2022-02-25
- Published: 2022-06-09
- Granted: 2023-07-11
- Earliest claimed: 2022-01-06
- Assignees: Jiangsu Riyu Photovoltaic New Material Technology Co. Ltd
- Applicants: Jiangsu Riyu Photovoltaic New Material Technology Co. Ltd
- Inventors: Li Yan; Song Xu; Rui Tian
- Web page: https://patentgrep.com/patent/US11697612B2

## CPC

- C03C 8/12: containing titanium or zirconium
- C03C 3/062: with less than 40% silica by weight
- C03C 3/07: containing lead
- C03C 3/122: {containing oxides of As, Sb, Bi, Mo, W, V, Te as glass formers}
- C03C 8/10: containing lead
- C03C 8/16: with vehicle or suspending agents, e.g. slip
- C03C 8/18: containing free metals
- H01B 1/16: the conductive material comprising metals or alloys
- H01B 1/22: the conductive material comprising metals or alloys
- H10F 77/211: {for photovoltaic cells}
- H10F 77/311: {for photovoltaic cells}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION

## Abstract

The present disclosure discloses a low LOI tellurium-lithium-silicon-zirconium frit system and a conductive paste and application thereof, and belongs to the field of conductive paste. In the low LOI tellurium-lithium-silicon-zirconium frit system, components of the frit are 24%-40% TeO2, 18%-24% Li2O, 4%-13% SiO2, 0-2% ZrO2, and a balance MOx, and M is one or a mixture of Na, K, Mg, Ca, Sr, Ti, V, Cr, Mo, W, Mn, Cu, Ag, Zn, Cd, B, Al, Ga, Tl, Ge, Pb, P, and Bi. There is no need to add additional surfactants, a viscosity change of the conductive paste prepared after standing for 30 days is less than 20%, the conductive paste has good stability, the water related weight loss of inorganic oxide of the conductive paste is less than 1.6%, and the application performance of the conductive paste is not affected after standing for 30 days.

## Claims

### Claim 1

A mixture comprising, in mol % 40% TeO2, 20% Li2O, 12% SiO2, 2% ZrO2, and 26% MOx, where MOx is one or a mixture of Na2O, K2O, MgO, CaO, SrO, TiO2, V2O5, Cr2O3, MoO3, WO3, MnO, CuO, Ag2O, ZnO, CdO, B2O3, Al2O3, Ga2O3, Tl2O3, GeO2, PbO, P2O5, and Bi2O3.

### Claim 2

The mixture where MOx is, in mol % 15% PbO 5% Bi2O3, 2% MgO, and 4% CaO.

### Claim 3

A mixture comprising, in mol %, 40% TeO2, 20% Li2O, 12% SiO2, 5% ZrO2, 14% PbO, 3% Bi2O3, 2% MgO, 4% CaO.